Final Magnetic Moment6.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.520 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMoP2O7 + Mo4P7O24 + MoO2 + Mo |
Band Gap3.444 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 291.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 163.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 81.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 163.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 81.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 81.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 254.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 81.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 215.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 291.7 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 205.5 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 245.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 81.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 163.9 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 215.6 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 291.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 254.3 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 291.7 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 215.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 163.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 145.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 254.3 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 0> | 291.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 107.8 |
Si (mp-149) | <1 0 0> | <0 1 0> | 291.7 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 163.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 291.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 215.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 81.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 291.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 163.9 |
Mg (mp-153) | <1 0 1> | <1 1 1> | 188.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 254.3 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 291.7 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 163.9 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 245.8 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 163.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 291.7 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 291.7 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 215.6 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 291.7 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 245.8 |
ZnO (mp-2133) | <0 0 1> | <1 1 0> | 254.3 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 163.9 |
SrTiO3 (mp-4651) | <1 1 1> | <0 0 1> | 215.6 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 163.9 |
Fe2O3 (mp-24972) | <1 1 0> | <1 0 0> | 245.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3(P2O7)2 (mp-32416) | 0.4428 | 0.033 | 3 |
Mn6P7O24 (mp-504168) | 0.4321 | 0.003 | 3 |
V6P7O24 (mp-32423) | 0.4493 | 0.036 | 3 |
P4W3O14 (mvc-1031) | 0.4638 | 0.315 | 3 |
Co3(P2O7)2 (mp-540500) | 0.4442 | 0.122 | 3 |
LiTi2P3O11 (mp-762500) | 0.2940 | 0.126 | 4 |
LiCr2P3O11 (mp-31661) | 0.2413 | 0.052 | 4 |
LiFe2P3O11 (mp-762652) | 0.3152 | 0.034 | 4 |
Cd5Mo2(P2O7)4 (mp-566657) | 0.2728 | 0.015 | 4 |
LiV2P3O11 (mp-697785) | 0.2963 | 0.229 | 4 |
CrO2 (mvc-11581) | 0.7457 | 0.166 | 2 |
Cr19O48 (mp-850874) | 0.7490 | 0.167 | 2 |
Cr5O12 (mp-19575) | 0.6973 | 0.142 | 2 |
VO2 (mvc-6918) | 0.7063 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.7365 | 0.281 | 2 |
LiCrPO4F (mp-770575) | 0.4791 | 0.054 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.4742 | 0.130 | 5 |
Na2ZrNi(P2O7)2 (mp-18984) | 0.3390 | 0.058 | 5 |
Na2ZrCo(P2O7)2 (mp-19187) | 0.3658 | 0.030 | 5 |
Na2ZrCo(P2O7)2 (mp-562673) | 0.3470 | 0.030 | 5 |
LiMnVP2(HO5)2 (mp-765066) | 0.5832 | 0.143 | 6 |
LiMnVP2(HO5)2 (mp-765378) | 0.5272 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-765074) | 0.5506 | 0.045 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5387 | 0.257 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.5150 | 0.072 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5915 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Li_sv Mo_pv P O |
Final Energy/Atom-7.1956 eV |
Corrected Energy-274.2248 eV
-274.2248 eV = -244.6504 eV (uncorrected energy) - 15.4504 eV (MP Anion Correction) - 14.1240 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)