Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.605 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.400 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 0 0> | <1 1 0> | 167.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 242.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 252.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 167.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 185.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 242.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 242.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 242.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 242.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 242.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 135.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 218.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 161.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 242.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 242.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 161.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 242.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 242.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 135.8 |
Si (mp-149) | <1 1 0> | <1 0 0> | 126.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 242.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 242.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 126.5 |
C (mp-48) | <1 1 1> | <0 1 1> | 135.8 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 0> | 218.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 218.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 126.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 167.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 242.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 252.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 185.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 161.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 167.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 242.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 252.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 218.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 109.0 |
C (mp-66) | <1 0 0> | <1 1 0> | 167.0 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 150.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 242.8 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 242.8 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 126.5 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 161.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 161.9 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 1> | 150.1 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 218.0 |
TiO2 (mp-390) | <1 0 0> | <1 0 1> | 150.1 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 242.8 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 218.0 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 1 1> | 135.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe(PO3)2 (mp-649683) | 0.4314 | 0.218 | 3 |
Mg(PO3)2 (mp-18620) | 0.4430 | 0.000 | 3 |
Mn(PO3)2 (mp-558444) | 0.4247 | 0.000 | 3 |
Co(PO3)2 (mp-547237) | 0.4429 | 0.064 | 3 |
Mn(PO3)2 (mp-629738) | 0.4251 | 0.000 | 3 |
LiP4WO12 (mp-763407) | 0.0580 | 0.071 | 4 |
LiTi(PO3)4 (mp-26113) | 0.1381 | 0.020 | 4 |
LiNb(PO3)4 (mp-26549) | 0.1646 | 0.067 | 4 |
LiMn(PO3)4 (mp-32007) | 0.1880 | 0.090 | 4 |
LiV(PO3)4 (mp-32492) | 0.1840 | 0.012 | 4 |
LiMnV(P2O7)2 (mp-764454) | 0.5303 | 0.007 | 5 |
LiVCr(P2O7)2 (mp-767608) | 0.5234 | 0.003 | 5 |
LiVFe(P2O7)2 (mp-767272) | 0.4950 | 0.001 | 5 |
LiMnV(PO4)3 (mp-770132) | 0.5203 | 0.041 | 5 |
LiMnV(P2O7)2 (mp-766110) | 0.5195 | 0.086 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4984 | 0.257 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.7022 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6308 | 0.331 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.6709 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6993 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Li_sv Mo_pv P O |
Final Energy/Atom-7.1504 eV |
Corrected Energy-562.6602 eV
-562.6602 eV = -514.8263 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 14.1240 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)