Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.570 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV2(PO4)3 |
Band Gap1.304 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 191.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 319.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 319.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 255.6 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 63.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 319.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 255.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 63.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 255.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 63.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 191.7 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 63.9 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 189.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 255.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 255.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 319.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 189.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 63.9 |
C (mp-48) | <0 0 1> | <1 0 1> | 189.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 255.6 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 255.6 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 255.6 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 191.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 191.7 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 178.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 255.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 319.5 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 319.5 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 191.7 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 319.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 63.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 319.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 319.5 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 189.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.9 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 255.6 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 319.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 191.7 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 191.7 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 63.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 255.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 319.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 191.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 191.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 127.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 191.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 255.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 319.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 191.7 |
C (mp-66) | <1 1 1> | <1 0 0> | 178.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.2270 | 0.344 | 3 |
VPO4 (mp-861584) | 0.2958 | 0.079 | 3 |
Co2(SO4)3 (mp-771299) | 0.4750 | 0.098 | 3 |
Cr3AgO8 (mp-560237) | 0.4356 | 0.000 | 3 |
TiPO4 (mp-779587) | 0.4006 | 0.077 | 3 |
LiCr2(PO4)3 (mp-31652) | 0.1145 | 0.038 | 4 |
LiMn2(PO4)3 (mp-32016) | 0.1317 | 0.019 | 4 |
LiTi2(PO4)3 (mp-18640) | 0.1119 | 0.001 | 4 |
V2Cu(PO4)3 (mp-761640) | 0.0783 | 0.014 | 4 |
Ti2Cu(PO4)3 (mp-772797) | 0.1143 | 0.009 | 4 |
Cr5O12 (mp-773920) | 0.5993 | 0.000 | 2 |
Mo4O11 (mp-622101) | 0.6961 | 0.017 | 2 |
Mo5O14 (mp-561240) | 0.7203 | 0.020 | 2 |
Mo4O11 (mp-565865) | 0.6512 | 0.025 | 2 |
V5O12 (mp-778252) | 0.6320 | 0.024 | 2 |
Ti3VCu2(PO4)6 (mp-761425) | 0.0904 | 0.016 | 5 |
Ti3Cu2P6WO24 (mp-763789) | 0.1196 | 0.072 | 5 |
Ti3NbCu2(PO4)6 (mp-776025) | 0.1144 | 0.061 | 5 |
Ti3CrCu2(PO4)6 (mp-775994) | 0.0882 | 0.061 | 5 |
V3FeCu2(PO4)6 (mp-765327) | 0.1226 | 0.039 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5002 | 0.068 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.1388 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4400 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.4301 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.4147 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.2309 eV |
Corrected Energy-283.5997 eV
Uncorrected energy = -260.3117 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -283.5997 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)