Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.487 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.110 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVPO5 + LiPO3 |
Band Gap1.081 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 264.3 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 143.7 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 163.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 172.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 277.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 272.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 233.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 272.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 272.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 190.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 194.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 152.2 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 215.6 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 277.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 266.4 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 272.0 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 198.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 190.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 272.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 155.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 114.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 310.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 198.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 155.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 264.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 287.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 272.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 152.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 287.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 304.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 215.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 215.6 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 272.0 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 272.0 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 233.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 163.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 264.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 190.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 152.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 172.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 349.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 266.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 266.4 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 66.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 38.1 |
BN (mp-984) | <1 0 1> | <0 1 1> | 163.2 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 66.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 230.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 272.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.25492 | 0.00000 | -0.71546 |
-1.25634 | -0.21932 | -1.57549 | 0.00000 | 0.59079 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.46266 | 0.00000 | -0.35298 |
Piezoelectric Modulus ‖eij‖max2.11133 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-2.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.71 | 0.00 | 0.25 |
0.00 | 5.39 | 0.00 |
0.25 | 0.00 | 6.84 |
Dielectric Tensor εij (total) |
||
---|---|---|
30.18 | 0.00 | 3.91 |
0.00 | 28.63 | 0.00 |
3.91 | 0.00 | 31.49 |
Polycrystalline dielectric constant
εpoly∞
5.98
|
Polycrystalline dielectric constant
εpoly
30.10
|
Refractive Index n2.45 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe7(P2O7)4 (mp-650224) | 0.5388 | 0.007 | 3 |
Ni7(P2O7)4 (mp-779819) | 0.4924 | 0.019 | 3 |
Ni6P7O24 (mp-504372) | 0.5590 | 0.009 | 3 |
Fe5(P3O11)2 (mp-31872) | 0.4974 | 0.366 | 3 |
Mn5(P3O11)2 (mp-31954) | 0.4076 | 0.065 | 3 |
Li3V2P5O18 (mp-697772) | 0.3991 | 0.092 | 4 |
LiNb(PO4)2 (mp-673070) | 0.1914 | 0.079 | 4 |
Li3Cr2P5O18 (mp-540364) | 0.4270 | 0.143 | 4 |
Li2CrP4O13 (mp-31739) | 0.4336 | 0.081 | 4 |
LiMnP2O7 (mp-849355) | 0.4021 | 0.004 | 4 |
LiCo2P4H3O16 (mp-762653) | 0.5455 | 0.141 | 5 |
LiFeP2HO8 (mp-762277) | 0.5313 | 0.268 | 5 |
LiV2P4(HO8)2 (mp-779883) | 0.5577 | 0.054 | 5 |
LiMgAl3(SeO4)6 (mp-532676) | 0.5791 | 0.010 | 5 |
LiV2P4(HO8)2 (mp-781070) | 0.5908 | 0.055 | 5 |
LiMnVP2(O4F)2 (mp-778336) | 0.3301 | 0.001 | 6 |
LiVFeP2(O4F)2 (mp-777635) | 0.4402 | 0.026 | 6 |
LiVCrP2(O4F)2 (mp-868574) | 0.5078 | 0.006 | 6 |
LiVCrP2(O4F)2 (mp-765305) | 0.5237 | 0.139 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.5273 | 0.111 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-6.9951 eV |
Corrected Energy-182.2742 eV
Uncorrected energy = -167.8822 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV
Corrected energy = -182.2742 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)