Final Magnetic Moment3.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVP2O7 + V(PO3)3 + LiPO3 + P |
Band Gap2.751 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 298.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 107.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 223.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 106.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 309.1 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 106.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 154.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 77.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 223.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 298.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 226.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 154.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 298.6 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 262.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 298.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 212.2 |
BN (mp-984) | <1 0 1> | <1 1 1> | 262.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 231.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 231.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 212.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 298.6 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 212.2 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 212.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 231.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.6 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 106.1 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 301.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 223.9 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 226.2 |
C (mp-66) | <1 1 0> | <1 0 1> | 107.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 223.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 149.3 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 309.1 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 298.6 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 1> | 214.9 |
Si (mp-149) | <1 0 0> | <1 0 0> | 154.5 |
C (mp-48) | <1 1 1> | <0 0 1> | 298.6 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 298.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 309.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 74.6 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 149.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 154.5 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 309.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 149.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 309.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 77.3 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 107.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 212.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 149.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.3283 | 0.020 | 3 |
Co3(P2O7)2 (mvc-12220) | 0.3523 | 0.122 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3451 | 0.098 | 3 |
Co3(P2O7)2 (mp-540500) | 0.3580 | 0.122 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.3502 | 0.366 | 3 |
LiCo(PO3)3 (mp-31583) | 0.0754 | 0.071 | 4 |
LiMn(PO3)3 (mp-762698) | 0.1657 | 0.190 | 4 |
LiNi(PO3)3 (mp-32380) | 0.1235 | 0.000 | 4 |
LiMn(PO3)3 (mp-19492) | 0.0728 | 0.186 | 4 |
LiFe(PO3)3 (mp-540112) | 0.0676 | 0.136 | 4 |
FeO2 (mvc-11999) | 0.6572 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.6417 | 0.166 | 2 |
Cr5O12 (mp-19575) | 0.6931 | 0.142 | 2 |
VO2 (mvc-6918) | 0.6567 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.7268 | 0.281 | 2 |
Li2VFe(P2O7)2 (mp-764318) | 0.3779 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-764248) | 0.3771 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-764239) | 0.3682 | 0.000 | 5 |
Li2VFe(P2O7)2 (mp-763862) | 0.3753 | 0.114 | 5 |
Li2VFe(P2O7)2 (mp-763861) | 0.3752 | 0.161 | 5 |
InBP2H5NO9 (mp-752709) | 0.6976 | 0.000 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5240 | 0.257 | 6 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.6535 | 0.030 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5981 | 0.331 | 6 |
AlBP2H5NO9 (mp-24757) | 0.6863 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5867 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.1992 eV |
Corrected Energy-435.1635 eV
-435.1635 eV = -403.1531 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)