material

VBrO

ID:

mp-27841


Material Details

Final Magnetic Moment
2.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.797 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.03 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.479 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmmn [59]
Hall
P 2 2ab 1ab
Point Group
mmm
Crystal System
orthorhombic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 0> <0 1 1> 0.000 102.5
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.004 244.1
GdScO3 (mp-5690) <1 0 1> <1 0 1> 0.004 112.1
TiO2 (mp-390) <1 1 0> <1 0 1> 0.005 261.5
PbS (mp-21276) <1 1 0> <0 1 1> 0.006 102.5
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.006 93.9
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.008 149.4
LiTaO3 (mp-3666) <1 1 0> <0 1 0> 0.008 125.7
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.009 112.1
Si (mp-149) <1 0 0> <1 0 1> 0.010 149.4
LiTaO3 (mp-3666) <0 0 1> <1 1 0> 0.013 46.9
NaCl (mp-22862) <1 1 0> <0 1 1> 0.013 136.6
CdWO4 (mp-19387) <1 1 0> <1 1 1> 0.013 244.1
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.016 267.7
KCl (mp-23193) <1 1 0> <1 0 0> 0.018 174.4
MgO (mp-1265) <1 1 1> <1 1 0> 0.020 93.9
ZrO2 (mp-2858) <0 1 1> <0 1 0> 0.021 157.1
LiGaO2 (mp-5854) <1 1 1> <1 1 0> 0.022 281.7
KTaO3 (mp-3614) <1 1 0> <0 1 1> 0.027 68.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.032 244.1
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.033 125.7
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.035 112.1
Te2W (mp-22693) <1 0 0> <1 0 1> 0.035 298.9
SrTiO3 (mp-4651) <1 0 1> <0 1 1> 0.036 273.3
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.037 186.8
KCl (mp-23193) <1 1 1> <1 1 0> 0.037 140.8
ZnO (mp-2133) <0 0 1> <0 1 1> 0.037 170.8
LiF (mp-1138) <1 1 1> <0 1 1> 0.038 170.8
LiNbO3 (mp-3731) <0 0 1> <1 1 0> 0.040 46.9
InSb (mp-20012) <1 1 0> <1 0 0> 0.041 313.9
LiNbO3 (mp-3731) <1 1 1> <1 0 1> 0.043 261.5
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.045 140.8
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.047 279.0
SiC (mp-11714) <1 0 1> <0 0 1> 0.048 160.6
Fe2O3 (mp-24972) <1 1 0> <0 1 0> 0.048 125.7
Te2W (mp-22693) <0 1 0> <0 0 1> 0.048 53.5
CdTe (mp-406) <1 1 0> <1 0 0> 0.051 313.9
Al (mp-134) <1 1 0> <0 1 1> 0.055 68.3
SiC (mp-8062) <1 1 1> <1 0 1> 0.055 336.2
SrTiO3 (mp-4651) <1 1 1> <0 0 1> 0.063 281.1
ZrO2 (mp-2858) <0 1 0> <1 1 1> 0.065 195.3
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.066 224.1
SiO2 (mp-6930) <0 0 1> <0 1 1> 0.067 170.8
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.068 174.0
InP (mp-20351) <1 1 1> <0 0 1> 0.071 307.8
SiC (mp-7631) <0 0 1> <1 0 0> 0.074 244.1
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.074 234.7
SiC (mp-11714) <0 0 1> <1 0 0> 0.075 244.1
SiO2 (mp-6930) <1 0 0> <1 1 1> 0.076 195.3
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.076 174.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.35 0.00 0.00
0.00 3.62 0.00
0.00 0.00 5.23
Dielectric Tensor εij (total)
10.15 0.00 0.00
0.00 4.28 0.00
0.00 0.00 9.85
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.40
Polycrystalline dielectric constant εpoly
(total)
8.09
Refractive Index n
2.10
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
InBrO (mp-27703) 0.1907 0.000 3
AlClO (mp-27863) 0.2743 0.000 3
TmBrO (mp-754526) 0.2875 0.010 3
ScBrO (mp-546279) 0.1757 0.000 3
ZrBrN (mp-570157) 0.3066 0.014 3
MgCl2 (mp-571387) 0.7377 0.142 2
RhN3 (mp-2118) 0.7088 0.432 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: V_pv Br O
Final Energy/Atom
-6.2245 eV
Corrected Energy
-42.1157 eV
-42.1157 eV = -37.3471 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 27010
Submitted by
User remarks:
  • Vanadium(III) oxide bromide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)