material

SrCu2O3

ID:

mp-3255

DOI:

10.17188/1206305


Tags: High pressure experimental phase Strontium dicuprate - HP

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.691 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.016 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.32 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SrCuO2 + CuO
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmmn [59]
Hall
P 2 2ab 1ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 95957 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.009 240.8
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.012 325.8
GdScO3 (mp-5690) <0 1 1> <0 0 1> 0.017 325.8
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.027 226.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.027 230.0
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.027 230.0
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.029 269.1
GdScO3 (mp-5690) <1 1 0> <1 0 1> 0.030 192.5
LiF (mp-1138) <1 1 1> <1 0 0> 0.034 230.0
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.035 164.9
C (mp-48) <1 1 1> <0 0 1> 0.041 170.0
MgAl2O4 (mp-3536) <1 1 1> <1 0 0> 0.041 230.0
Ge (mp-32) <1 1 1> <0 1 1> 0.042 174.4
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.046 325.8
Ga2O3 (mp-886) <1 1 -1> <1 0 1> 0.051 240.6
PbS (mp-21276) <1 0 0> <1 0 1> 0.055 144.4
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.055 48.1
Te2Mo (mp-602) <0 0 1> <0 1 1> 0.062 43.6
TeO2 (mp-2125) <1 0 1> <1 1 0> 0.062 308.9
TiO2 (mp-390) <0 0 1> <1 0 1> 0.064 144.4
Mg (mp-153) <0 0 1> <1 0 0> 0.067 230.0
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.067 339.9
MgO (mp-1265) <1 0 0> <1 0 1> 0.068 144.4
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.070 322.0
ZnO (mp-2133) <1 0 0> <1 1 0> 0.074 123.6
TbScO3 (mp-31119) <1 1 0> <1 0 1> 0.080 192.5
GaAs (mp-2534) <1 1 1> <0 1 1> 0.081 174.4
NaCl (mp-22862) <1 1 0> <0 0 1> 0.090 184.1
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.091 226.6
SiO2 (mp-6930) <1 0 1> <0 1 1> 0.100 174.4
Ni (mp-23) <1 1 0> <0 0 1> 0.106 70.8
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.107 46.0
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 0.109 206.2
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.110 85.0
ZnSe (mp-1190) <1 1 1> <0 1 1> 0.113 174.4
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.117 144.4
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.119 297.4
WS2 (mp-224) <1 0 1> <0 0 1> 0.119 226.6
AlN (mp-661) <0 0 1> <0 0 1> 0.125 141.6
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.127 283.3
NaCl (mp-22862) <1 0 0> <1 0 1> 0.131 96.3
C (mp-48) <0 0 1> <0 0 1> 0.134 155.8
GaSe (mp-1943) <1 0 0> <0 1 0> 0.136 206.2
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.136 325.8
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.138 164.9
GaSe (mp-1943) <0 0 1> <1 0 0> 0.142 230.0
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.146 297.4
BN (mp-984) <0 0 1> <0 0 1> 0.147 155.8
AlN (mp-661) <1 0 0> <0 0 1> 0.150 127.5
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.155 184.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
239 136 25 0 0 0
136 258 42 0 0 0
25 42 98 0 0 0
0 0 0 17 0 0
0 0 0 0 26 0
0 0 0 0 0 81
Compliance Tensor Sij (10-12Pa-1)
6 -3.1 -0.2 0 0 0
-3.1 5.8 -1.7 0 0 0
-0.2 -1.7 11 0 0 0
0 0 0 58.1 0 0
0 0 0 0 38.6 0
0 0 0 0 0 12.4
Shear Modulus GV
51 GPa
Bulk Modulus KV
111 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
78 GPa
Shear Modulus GVRH
43 GPa
Bulk Modulus KVRH
95 GPa
Elastic Anisotropy
2.87
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrCu2O3 (mp-5938) 0.2020 0.018 3
NaCu2O3 (mp-754631) 0.5045 0.074 3
Sr2Cu3O5 (mp-552089) 0.2734 0.010 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Cu_pv O
Final Energy/Atom
-5.4615 eV
Corrected Energy
-69.6597 eV
Uncorrected energy = -65.5377 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -69.6597 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 99042
  • 95957
Submitted by
User remarks:
  • High pressure experimental phase
  • Strontium dicuprate - HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)