Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.833 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 274.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 211.2 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 252.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 163.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 261.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 222.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 312.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 241.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 321.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 193.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 52.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 133.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 133.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 341.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 261.4 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 160.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 133.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 252.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 200.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 160.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 297.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 252.5 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 211.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 200.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 261.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 312.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 74.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 163.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 133.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 149.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 264.0 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 211.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 237.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 158.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 219.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 112.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 133.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 211.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 160.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 252.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 112.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 237.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 160.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er(CoSi)2 (mp-3239) | 0.0104 | 0.000 | 3 |
Ho(CoSi)2 (mp-5835) | 0.0192 | 0.000 | 3 |
Dy(CoSi)2 (mp-5976) | 0.0300 | 0.000 | 3 |
Y(CoSi)2 (mp-5129) | 0.0374 | 0.000 | 3 |
Ca(GeRh)2 (mp-16261) | 0.0204 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.5364 | 0.000 | 4 |
CaGa4 (mp-1976) | 0.2399 | 0.000 | 2 |
SrAl4 (mp-2775) | 0.1851 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.2452 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.1255 | 0.000 | 2 |
BaIn4 (mp-22687) | 0.2423 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Co Si |
Final Energy/Atom-6.7408 eV |
Corrected Energy-33.5622 eV
Uncorrected energy = -33.7042 eV
Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV
Corrected energy = -33.5622 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)