Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.041 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.138 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 263.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 263.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 87.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 87.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 87.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 263.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 175.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 87.9 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 263.8 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 263.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 87.9 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 175.9 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 87.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 263.8 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 175.9 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 87.9 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 87.9 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 263.8 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 263.8 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 263.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm3(Bi7Te12)2 (mp-675353) | 0.4526 | 0.124 | 3 |
Dy5AgS8 (mp-35512) | 0.4704 | 0.033 | 3 |
K2SrCl4 (mp-674465) | 0.4091 | 0.027 | 3 |
Dy14(PbS8)3 (mp-675822) | 0.4591 | 0.049 | 3 |
Ho14(PbS8)3 (mp-675425) | 0.4295 | 0.059 | 3 |
TiTlCuTe3 (mp-9344) | 0.6917 | 0.000 | 4 |
Rb2CeCu3Te5 (mp-581778) | 0.7453 | 0.093 | 4 |
Ba20As13 (mp-685008) | 0.2888 | 0.000 | 2 |
Lu2S3 (mp-32642) | 0.2836 | 0.063 | 2 |
Y2S3 (mp-32891) | 0.3540 | 0.036 | 2 |
Tm2S3 (mp-32933) | 0.3242 | 0.063 | 2 |
Ba3P2 (mp-32606) | 0.1869 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv P |
Final Energy/Atom-4.2199 eV |
Corrected Energy-168.7980 eV
-168.7980 eV = -168.7980 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)