Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.382 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.063 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLu2S3 |
Band Gap2.078 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 133.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 66.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 267.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 267.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 133.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 66.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 267.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 267.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 267.6 |
C (mp-48) | <1 0 1> | <0 0 1> | 200.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 200.7 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 66.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 133.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 267.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 66.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 267.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 133.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 267.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 66.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 133.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 267.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.6 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 267.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 267.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 133.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 200.0 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 66.9 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 66.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 133.8 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 267.6 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 200.0 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 267.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd10US16 (mp-685926) | 0.3016 | 0.028 | 3 |
Pr10US16 (mp-675336) | 0.3350 | 0.028 | 3 |
Ce10US16 (mp-676880) | 0.3442 | 0.018 | 3 |
Tb14(PbSe8)3 (mp-676110) | 0.3488 | 0.043 | 3 |
Ho14(PbS8)3 (mp-675425) | 0.3452 | 0.059 | 3 |
Ho2S3 (mp-32787) | 0.1330 | 0.035 | 2 |
Dy2S3 (mp-32826) | 0.1308 | 0.025 | 2 |
Tm2Se3 (mp-32850) | 0.1385 | 0.088 | 2 |
Y2S3 (mp-32891) | 0.1036 | 0.036 | 2 |
Tm2S3 (mp-32933) | 0.0587 | 0.063 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 S |
Final Energy/Atom-6.2742 eV |
Corrected Energy-266.8895 eV
-266.8895 eV = -250.9664 eV (uncorrected energy) - 15.9230 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)