Final Magnetic Moment0.062 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.237 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe8Ir3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 219.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 292.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 219.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 292.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 219.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 73.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 180.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 127.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 292.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 292.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 219.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 180.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 73.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 292.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 219.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 292.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 73.2 |
LiNbO3 (mp-3731) | <1 1 1> | <0 1 1> | 127.5 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 1> | 127.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 219.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 219.6 |
TeO2 (mp-2125) | <1 1 0> | <1 1 1> | 194.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 219.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 219.6 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 207.4 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 103.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 292.8 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 180.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 219.6 |
TiO2 (mp-2657) | <1 1 0> | <1 1 1> | 194.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 219.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 219.6 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 73.2 |
MoSe2 (mp-1634) | <1 1 0> | <1 1 0> | 180.0 |
Si (mp-149) | <1 1 1> | <0 0 1> | 219.6 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 219.6 |
C (mp-48) | <1 0 1> | <0 0 1> | 292.8 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 180.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 219.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 292.8 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 146.4 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 146.4 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 180.0 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 292.8 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 219.6 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 103.7 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 180.0 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 180.0 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 292.8 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 292.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Ti3O8 (mvc-2955) | 0.6840 | 0.000 | 3 |
Na2Mn3O7 (mp-19080) | 0.6586 | 0.000 | 3 |
Li2MnF5 (mp-762998) | 0.6827 | 0.248 | 3 |
KMn2O4 (mp-1080245) | 0.6490 | 0.170 | 3 |
Na4Ge5O12 (mp-1094119) | 0.6805 | 0.158 | 3 |
Li4V4(OF3)3 (mp-765901) | 0.6737 | 0.101 | 4 |
Li4Mn(TeO4)3 (mp-771794) | 0.6985 | 0.065 | 4 |
Ta2Zn2CrO8 (mvc-2652) | 0.6924 | 0.160 | 4 |
Ca4Ni5(TeO6)3 (mvc-3151) | 0.6717 | 0.193 | 4 |
Nb2Zn2WO8 (mvc-551) | 0.6660 | 0.157 | 4 |
Te8Rh3 (mp-7273) | 0.6394 | 0.000 | 2 |
Ir3Se8 (mp-9888) | 0.7183 | 0.000 | 2 |
Rh3Se8 (mp-1407) | 0.7325 | 0.000 | 2 |
Mn5O8 (mp-715008) | 0.7304 | 0.009 | 2 |
Rh3Se8 (mp-32861) | 0.7388 | 0.007 | 2 |
Li4MnSb(WO6)2 (mp-779994) | 0.6936 | 0.041 | 5 |
Li4SbTe2WO12 (mp-765930) | 0.6638 | 0.086 | 5 |
Li4MnNb(WO6)2 (mp-771868) | 0.6940 | 0.027 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.6620 | 0.036 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.6828 | 0.076 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Ir |
Final Energy/Atom-4.9334 eV |
Corrected Energy-162.8035 eV
-162.8035 eV = -162.8035 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)