Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.806 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToEr2Se3 |
Band Gap1.622 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 298.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 223.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 298.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 298.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 149.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 223.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 298.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 298.3 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 223.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 223.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 74.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 149.2 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 74.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 298.3 |
Si (mp-149) | <1 0 0> | <0 0 1> | 149.2 |
Au (mp-81) | <1 0 0> | <0 0 1> | 298.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 74.6 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 298.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 223.8 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 149.2 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 149.2 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 298.3 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 74.6 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 298.3 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 223.8 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 298.3 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 149.2 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 74.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MoSeS2Cl5 (mp-560907) | 0.7413 | 0.000 | 4 |
Tm2Se3 (mp-32850) | 0.0905 | 0.000 | 2 |
Er2S3 (mp-684708) | 0.1126 | 0.041 | 2 |
Tb2Se3 (mp-685003) | 0.0876 | 0.024 | 2 |
Ho2Se3 (mp-685041) | 0.0650 | 0.062 | 2 |
Y2Se3 (mp-673656) | 0.0673 | 0.000 | 2 |
La10US16 (mp-675741) | 0.3211 | 0.051 | 3 |
Nd10US16 (mp-685926) | 0.2347 | 0.045 | 3 |
Pr10US16 (mp-675336) | 0.2655 | 0.045 | 3 |
Ce10US16 (mp-676880) | 0.2627 | 0.066 | 3 |
Tb14(PbSe8)3 (mp-676110) | 0.2988 | 0.043 | 3 |
Rb (mp-640416) | 0.6635 | 0.029 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Se |
Final Energy/Atom-5.7271 eV |
Corrected Energy-229.0859 eV
-229.0859 eV = -229.0859 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)