material

BAsO4

ID:

mp-3277

DOI:

10.17188/1206376


Tags: Boron arsenate(V)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.143 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.441 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4 [82]
Hall
I 4
Point Group
4
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 26891 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 0 0> <1 1 1> 0.000 147.9
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.000 273.4
GaP (mp-2490) <1 0 0> <0 0 1> 0.001 273.4
Cu (mp-30) <1 0 0> <0 0 1> 0.004 105.1
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.006 105.1
TiO2 (mp-390) <0 0 1> <1 0 0> 0.006 189.3
LiGaO2 (mp-5854) <0 1 0> <1 1 1> 0.010 98.6
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.013 105.1
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.013 283.9
LiF (mp-1138) <1 0 0> <0 0 1> 0.013 84.1
SiC (mp-7631) <1 0 1> <1 0 1> 0.016 189.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.024 189.3
Ge (mp-32) <1 0 0> <0 0 1> 0.028 168.2
BN (mp-984) <0 0 1> <1 1 0> 0.029 178.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.030 189.3
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.030 178.4
C (mp-48) <1 1 0> <1 0 1> 0.034 265.4
LiGaO2 (mp-5854) <1 0 1> <1 0 1> 0.034 227.5
Mg (mp-153) <1 1 0> <1 0 0> 0.038 315.4
CdS (mp-672) <1 1 0> <1 0 0> 0.039 252.3
Si (mp-149) <1 0 0> <0 0 1> 0.040 273.4
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.042 273.4
GaAs (mp-2534) <1 0 0> <0 0 1> 0.050 168.2
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.051 265.4
C (mp-48) <1 0 0> <0 0 1> 0.053 231.3
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.057 347.0
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.061 178.4
SiC (mp-11714) <1 0 0> <1 0 1> 0.062 341.2
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.066 189.3
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.067 168.2
GaTe (mp-542812) <1 0 0> <1 0 1> 0.069 265.4
MgAl2O4 (mp-3536) <1 1 0> <1 0 1> 0.069 189.5
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.071 273.4
LiF (mp-1138) <1 1 0> <1 0 1> 0.071 189.5
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.071 168.2
AlN (mp-661) <1 1 1> <1 0 0> 0.072 347.0
ZnO (mp-2133) <0 0 1> <0 0 1> 0.072 147.2
Mg (mp-153) <1 0 1> <1 1 0> 0.075 223.0
ZnO (mp-2133) <1 1 1> <1 0 1> 0.077 189.5
Ge (mp-32) <1 1 0> <1 0 1> 0.086 189.5
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.087 75.8
BN (mp-984) <1 1 0> <1 0 1> 0.090 265.4
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.090 252.3
GaN (mp-804) <1 1 0> <1 0 0> 0.098 315.4
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.099 273.4
BN (mp-984) <1 0 1> <1 1 1> 0.102 246.6
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.103 336.5
CdSe (mp-2691) <1 0 0> <1 0 0> 0.103 189.3
TePb (mp-19717) <1 0 0> <0 0 1> 0.106 42.1
WS2 (mp-224) <1 0 1> <0 0 1> 0.106 189.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
105 -16 38 0 0 -1
-16 105 38 0 0 1
38 38 99 0 0 0
0 0 0 51 0 0
0 0 0 0 51 0
-1 1 0 0 0 37
Compliance Tensor Sij (10-12Pa-1)
12.6 4.3 -6.5 0 0 0.2
4.3 12.6 -6.5 0 0 -0.2
-6.5 -6.5 15.1 0 0 0
0 0 0 19.7 0 0
0 0 0 0 19.7 0
0.2 -0.2 0 0 0 27.4
Shear Modulus GV
44 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
38 GPa
Bulk Modulus KR
44 GPa
Shear Modulus GVRH
41 GPa
Bulk Modulus KVRH
46 GPa
Elastic Anisotropy
0.93
Poisson's Ratio
0.16

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.02249 0.15198 0.00000
0.00000 0.00000 0.00000 -0.15198 -0.02249 0.00000
0.37172 -0.37172 0.00000 0.00000 0.00000 -0.34298
Piezoelectric Modulus ‖eijmax
0.62768 C/m2
Crystallographic Direction vmax
0.00000
0.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.03 0.00 0.00
0.00 3.03 0.00
0.00 0.00 3.12
Dielectric Tensor εij (total)
5.50 0.00 0.00
0.00 5.50 0.00
0.00 0.00 6.49
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.06
Polycrystalline dielectric constant εpoly
(total)
5.83
Refractive Index n
1.75
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CoPO4 (mp-689943) 0.3040 0.223 3
CoPO4 (mp-767355) 0.3255 0.207 3
GaAsO4 (mp-3996) 0.3162 0.000 3
LiFeF4 (mp-777020) 0.3305 0.095 3
NiPO4 (mp-697731) 0.3314 0.151 3
Rb2Al2Si3O10 (mp-975622) 0.6943 0.009 4
K2Ge3(BO5)2 (mp-560019) 0.7319 0.000 4
KGe2BO6 (mp-556463) 0.6695 0.000 4
LiB(SO4)2 (mp-1020106) 0.6823 0.000 4
GeO2 (mp-7812) 0.3614 0.001 2
GeO2 (mp-223) 0.3704 0.000 2
CO2 (mp-1077316) 0.3566 0.450 2
GeO2 (mp-733) 0.3752 0.000 2
SiO2 (mp-557591) 0.3657 0.066 2
RbZnB(PO4)2 (mp-557658) 0.5080 0.000 5
CsZnB(PO4)2 (mp-560244) 0.5526 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: B As O
Final Energy/Atom
-6.8627 eV
Corrected Energy
-43.9239 eV
Uncorrected energy = -41.1759 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -43.9239 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 413438
  • 26891
Submitted by
User remarks:
  • Boron arsenate(V)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)