Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.437 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2S3 |
Band Gap1.925 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 0 1> | 209.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 279.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 279.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 279.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 279.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 279.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 209.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 139.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.8 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 279.1 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 209.3 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 279.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.8 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 279.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 209.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 279.1 |
Si (mp-149) | <1 0 0> | <0 0 1> | 279.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 69.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 139.6 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 279.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 279.1 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 279.1 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 279.1 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 69.8 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 279.1 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 139.6 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 279.1 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 279.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd10US16 (mp-685926) | 0.2513 | 0.028 | 3 |
Pr10US16 (mp-675336) | 0.2714 | 0.028 | 3 |
Ce10US16 (mp-676880) | 0.2800 | 0.018 | 3 |
La10US16 (mp-675741) | 0.3130 | 0.033 | 3 |
Tb14(PbSe8)3 (mp-676110) | 0.3420 | 0.043 | 3 |
Gd2S3 (mp-684712) | 0.0796 | 0.021 | 2 |
Er2S3 (mp-684708) | 0.0718 | 0.041 | 2 |
Ho2S3 (mp-32787) | 0.0441 | 0.035 | 2 |
Dy2S3 (mp-32826) | 0.0361 | 0.025 | 2 |
Tm2S3 (mp-32933) | 0.0535 | 0.063 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv S |
Final Energy/Atom-7.1070 eV |
Corrected Energy-300.2024 eV
-300.2024 eV = -284.2793 eV (uncorrected energy) - 15.9230 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)