material

CaPd3O4

ID:

mp-3315

DOI:

10.17188/1206517


Tags: Calcium tripalladium oxide Calcium tripalladium tetraoxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.524 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.021 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 16538 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaP (mp-2490) <1 0 0> <1 0 0> 0.000 272.9
C (mp-66) <1 1 0> <1 1 0> 0.001 144.7
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.002 177.2
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.004 272.9
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.004 136.4
Mg (mp-153) <0 0 1> <1 1 1> 0.006 236.3
Cu (mp-30) <1 0 0> <1 0 0> 0.007 170.6
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.007 307.0
Mg (mp-153) <1 1 1> <1 0 0> 0.009 272.9
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.009 272.9
WS2 (mp-224) <1 1 1> <1 1 1> 0.010 236.3
AlN (mp-661) <0 0 1> <1 1 1> 0.013 59.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.013 307.0
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.015 307.0
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.016 307.0
CdSe (mp-2691) <1 0 0> <1 0 0> 0.025 307.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.026 307.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.031 144.7
GaN (mp-804) <1 0 0> <1 1 0> 0.033 337.7
WS2 (mp-224) <1 1 0> <1 1 1> 0.034 236.3
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.037 236.3
WS2 (mp-224) <0 0 1> <1 1 1> 0.038 236.3
Ni (mp-23) <1 1 0> <1 1 0> 0.044 193.0
Ag (mp-124) <1 1 1> <1 0 0> 0.045 238.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.046 307.0
LiGaO2 (mp-5854) <0 1 0> <1 1 1> 0.053 295.4
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.054 272.9
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.068 289.4
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.069 177.2
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.073 96.5
Te2W (mp-22693) <0 1 1> <1 1 0> 0.077 289.4
PbSe (mp-2201) <1 0 0> <1 0 0> 0.080 307.0
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.083 170.6
GaN (mp-804) <1 1 1> <1 0 0> 0.086 272.9
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.090 136.4
TePb (mp-19717) <1 0 0> <1 0 0> 0.092 170.6
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.098 136.4
Au (mp-81) <1 1 1> <1 0 0> 0.100 238.8
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.104 204.7
C (mp-48) <1 1 1> <1 1 1> 0.108 236.3
SiC (mp-8062) <1 0 0> <1 0 0> 0.109 170.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.109 272.9
C (mp-48) <1 0 0> <1 0 0> 0.125 307.0
Si (mp-149) <1 0 0> <1 0 0> 0.137 272.9
GaTe (mp-542812) <1 0 0> <1 1 1> 0.137 177.2
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.138 144.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.146 272.9
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.149 307.0
BN (mp-984) <0 0 1> <1 1 0> 0.158 193.0
Ag (mp-124) <1 1 0> <1 1 0> 0.159 48.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
259 119 119 0 0 0
119 259 119 0 0 0
119 119 259 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 47
Compliance Tensor Sij (10-12Pa-1)
5.4 -1.7 -1.7 0 0 0
-1.7 5.4 -1.7 0 0 0
-1.7 -1.7 5.4 0 0 0
0 0 0 21.4 0 0
0 0 0 0 21.4 0
0 0 0 0 0 21.4
Shear Modulus GV
56 GPa
Bulk Modulus KV
166 GPa
Shear Modulus GR
54 GPa
Bulk Modulus KR
166 GPa
Shear Modulus GVRH
55 GPa
Bulk Modulus KVRH
166 GPa
Elastic Anisotropy
0.20
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LaPd3S4 (mp-2889) 0.0000 0.000 3
NaPt3O4 (mp-20285) 0.0000 0.000 3
NdPd3S4 (mp-15227) 0.0000 0.000 3
EuPd3S4 (mp-20961) 0.0000 0.000 3
CdPd3O4 (mp-13675) 0.0000 0.004 3
NaLu(Pd3O4)2 (mp-6533) 0.4878 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Pd O
Final Energy/Atom
-5.8380 eV
Corrected Energy
-98.9038 eV
Uncorrected energy = -93.4078 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Corrected energy = -98.9038 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 186819
  • 16538
  • 27502
Submitted by
User remarks:
  • Calcium tripalladium tetraoxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)