Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.207 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTbAgS2 + Tb2S3 |
Band Gap1.716 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 278.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 140.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 209.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 278.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 280.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 140.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 242.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 278.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.7 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 98.8 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 121.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 121.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 296.4 |
Al (mp-134) | <1 0 0> | <1 1 1> | 242.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 209.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 139.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 280.2 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 296.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.7 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 98.8 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 121.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 278.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 278.6 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 98.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 209.0 |
C (mp-66) | <1 1 0> | <1 0 1> | 197.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 1> | 242.2 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 280.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 209.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 278.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 278.6 |
Au (mp-81) | <1 1 0> | <1 0 1> | 98.8 |
Au (mp-81) | <1 1 1> | <1 1 1> | 121.1 |
C (mp-48) | <1 0 0> | <1 0 0> | 210.2 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 278.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.7 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 98.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.7 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 280.2 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 296.4 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 278.6 |
SiC (mp-8062) | <1 1 0> | <1 0 1> | 296.4 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 197.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 278.6 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 278.6 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 121.1 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 98.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 1> | 296.4 |
Au (mp-81) | <1 0 0> | <0 0 1> | 69.7 |
GaTe (mp-542812) | <0 0 1> | <1 0 1> | 296.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.35613 | 0.13544 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.13543 | 0.35613 | 0.00000 |
0.00798 | -0.00797 | 0.00000 | 0.00000 | 0.00000 | 0.39228 |
Piezoelectric Modulus ‖eij‖max0.39244 C/m2 |
Crystallographic Direction vmax |
---|
-0.00000 |
1.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.76 | 0.00 | 0.00 |
-0.00 | 8.76 | -0.00 |
0.00 | -0.00 | 8.62 |
Dielectric Tensor εij (total) |
||
---|---|---|
25.66 | 0.00 | 0.00 |
-0.00 | 25.66 | -0.00 |
0.00 | -0.00 | 23.61 |
Polycrystalline dielectric constant
εpoly∞
8.71
|
Polycrystalline dielectric constant
εpoly
24.98
|
Refractive Index n2.95 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd5AgSe8 (mp-685977) | 0.0897 | 0.025 | 3 |
Dy5AgS8 (mp-35512) | 0.0612 | 0.033 | 3 |
Nd5AgS8 (mp-37449) | 0.0872 | 0.021 | 3 |
Sm5AgS8 (mp-37923) | 0.0528 | 0.022 | 3 |
Gd5AgS8 (mp-676156) | 0.0659 | 0.394 | 3 |
Pr4Ge3 (mp-570606) | 0.3691 | 0.000 | 2 |
Hf3N4 (mp-11660) | 0.3710 | 0.069 | 2 |
Pr4As3 (mp-2365) | 0.3695 | 0.020 | 2 |
Eu4As3 (mp-20995) | 0.3779 | 0.000 | 2 |
La4As3 (mp-568959) | 0.3804 | 0.010 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Ag S |
Final Energy/Atom-6.0491 eV |
Corrected Energy-89.9953 eV
-89.9953 eV = -84.6876 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)