Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.493 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.876 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 20294 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 0 0> <0 0 1> 0.001 77.7
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.003 31.1
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.010 62.1
GaSb (mp-1156) <1 0 0> <0 0 1> 0.011 77.7
Au (mp-81) <1 0 0> <0 0 1> 0.012 139.8
GaN (mp-804) <0 0 1> <0 0 1> 0.012 170.8
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.019 279.6
CsI (mp-614603) <1 0 0> <0 0 1> 0.023 62.1
CdSe (mp-2691) <1 0 0> <0 0 1> 0.024 77.7
Au (mp-81) <1 1 1> <1 0 0> 0.024 242.5
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.043 233.0
Ag (mp-124) <1 0 0> <0 0 1> 0.060 139.8
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.063 217.4
Ni (mp-23) <1 0 0> <0 0 1> 0.064 62.1
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.064 228.6
BN (mp-984) <1 0 1> <0 0 1> 0.070 201.9
Ag (mp-124) <1 1 1> <1 0 0> 0.084 242.5
SiC (mp-8062) <1 0 0> <0 0 1> 0.101 77.7
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.114 217.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.147 139.8
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.154 77.7
InP (mp-20351) <1 0 0> <0 0 1> 0.167 139.8
GaP (mp-2490) <1 1 0> <0 0 1> 0.174 217.4
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.174 155.3
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.175 62.1
InAs (mp-20305) <1 0 0> <0 0 1> 0.177 77.7
Ag (mp-124) <1 1 0> <1 0 0> 0.185 242.5
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.189 217.4
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.189 295.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.193 170.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.194 170.8
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.197 77.7
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.206 279.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.208 161.7
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.223 201.9
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.226 310.6
ZnO (mp-2133) <1 1 0> <0 0 1> 0.244 357.2
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.255 114.3
GaN (mp-804) <1 0 0> <0 0 1> 0.263 170.8
Au (mp-81) <1 1 0> <1 0 0> 0.272 242.5
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.278 62.1
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.280 242.5
Mg (mp-153) <1 0 1> <0 0 1> 0.281 264.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.293 326.1
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.294 31.1
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.306 186.4
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.325 139.8
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.328 31.1
LiF (mp-1138) <1 1 0> <0 0 1> 0.329 264.0
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.332 228.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
265 75 84 0 0 0
75 265 84 0 0 0
84 84 246 0 0 0
0 0 0 75 0 0
0 0 0 0 75 0
0 0 0 0 0 91
Compliance Tensor Sij (10-12Pa-1)
4.4 -0.9 -1.2 0 0 0
-0.9 4.4 -1.2 0 0 0
-1.2 -1.2 4.9 0 0 0
0 0 0 13.3 0 0
0 0 0 0 13.3 0
0 0 0 0 0 11
Shear Modulus GV
84 GPa
Bulk Modulus KV
140 GPa
Shear Modulus GR
83 GPa
Bulk Modulus KR
140 GPa
Shear Modulus GVRH
83 GPa
Bulk Modulus KVRH
140 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr3Fe2O7 (mp-18820) 0.0313 0.000 3
Ba3Zr2O7 (mp-755895) 0.0489 0.000 3
Ba3Hf2O7 (mp-754128) 0.0866 0.000 3
K3Mn2F7 (mp-554144) 0.0695 0.000 3
Sr3Mn2O7 (mp-19070) 0.0678 0.028 3
SrEu2Al2O7 (mp-983228) 0.4710 0.047 4
Ba3SrTa2O9 (mp-7980) 0.6804 0.015 4
SrGd2Al2O7 (mp-545404) 0.7225 0.029 4
K2RbMn2F7 (mp-558227) 0.1110 0.000 4
K2RbMn2F7 (mp-613298) 0.1062 0.000 4
Ba3CaZrWO9 (mp-736122) 0.7139 0.175 5
Ba6Tb3Nb(SnO9)2 (mp-686370) 0.7018 0.084 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Ti_pv O
Final Energy/Atom
-7.7169 eV
Corrected Energy
-97.4112 eV
Uncorrected energy = -92.6022 eV Composition-based energy adjustment (-0.687 eV/atom x 7.0 atoms) = -4.8090 eV Corrected energy = -97.4112 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 20294
  • 63704
  • 34629
Submitted by
User remarks:
  • Tristrontium dititanium oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)