Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.314 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbTlO3 + Nb2O5 + Tl2O3 |
Band Gap0.048 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 164.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 164.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 232.6 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 164.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 232.6 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 116.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 164.4 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 116.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 232.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 232.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 116.3 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 164.4 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 232.6 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 164.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 1 0> | 164.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 116.3 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 116.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 164.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 116.3 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 164.4 |
LiAlO2 (mp-3427) | <0 0 1> | <1 1 0> | 164.4 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 164.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 164.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 116.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 164.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 164.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 164.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2Os2O7 (mp-22089) | 0.0439 | 0.034 | 3 |
Ta2Sn2O7 (mp-3593) | 0.0030 | 0.078 | 3 |
Nb2Sn2O7 (mp-556524) | 0.0577 | 0.087 | 3 |
Nb2Hg2O7 (mp-13803) | 0.0638 | 0.004 | 3 |
Cd2Re2O7 (mp-16783) | 0.0650 | 0.043 | 3 |
La2Nb2N2O5 (mp-775911) | 0.4017 | 0.071 | 4 |
Mn2Hg2SF6 (mp-600275) | 0.4145 | 0.465 | 4 |
Cu2Hg2SF6 (mp-6820) | 0.1806 | 0.000 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.3358 | 0.000 | 4 |
Ni2Hg2SF6 (mp-559259) | 0.2089 | 0.028 | 4 |
YbTiCdSbO7 (mp-677151) | 0.4282 | 0.073 | 5 |
NaCaNb2O6F (mp-42255) | 0.2774 | 0.005 | 5 |
LiCaTa2O6F (mp-39511) | 0.2529 | 0.030 | 5 |
Ca2Nd2Nb3FeO14 (mvc-16570) | 0.4153 | 0.111 | 5 |
Ca2Nd2Nb3FeO14 (mp-40206) | 0.3871 | 0.111 | 5 |
NaYbTiNbO6F (mp-684861) | 0.4502 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.5456 | 0.035 | 6 |
NaEuTiNbO6F (mp-43048) | 0.4498 | 0.021 | 6 |
NaCeTiNbO6F (mp-43055) | 0.5361 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.5410 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Tl_d O |
Final Energy/Atom-7.2813 eV |
Corrected Energy-169.8075 eV
Uncorrected energy = -160.1895 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -169.8075 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)