material

Y(CuSi)2

ID:

mp-3390

DOI:

10.17188/1206679


Tags: Copper yttrium silicide (2/1/2) Yttrium copper silicide (1/2/2)

Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.598 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.75 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 0 0> <0 0 1> 0.000 141.9
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.000 157.7
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.001 78.8
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.034 63.1
LiTaO3 (mp-3666) <1 0 0> <1 1 1> 0.045 292.1
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.056 220.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.059 63.1
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.069 220.7
LiNbO3 (mp-3731) <1 0 0> <1 1 1> 0.081 292.1
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.081 278.4
LaAlO3 (mp-2920) <1 0 1> <1 0 1> 0.099 299.5
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.110 198.8
C (mp-66) <1 0 0> <0 0 1> 0.110 63.1
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.114 63.1
Ag (mp-124) <1 1 0> <0 0 1> 0.122 268.0
C (mp-48) <1 1 1> <1 0 1> 0.136 171.1
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.160 236.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.162 15.8
PbS (mp-21276) <1 0 0> <0 0 1> 0.164 141.9
ZnO (mp-2133) <1 1 1> <1 1 0> 0.167 225.0
AlN (mp-661) <0 0 1> <0 0 1> 0.171 315.4
Au (mp-81) <1 1 0> <0 0 1> 0.173 268.0
PbSe (mp-2201) <1 0 0> <0 0 1> 0.175 78.8
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.188 31.5
ZnO (mp-2133) <1 0 0> <1 0 0> 0.201 159.1
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.206 63.1
AlN (mp-661) <1 1 0> <1 0 1> 0.208 213.9
CdS (mp-672) <0 0 1> <1 0 0> 0.214 278.4
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.229 225.0
GaSb (mp-1156) <1 0 0> <0 0 1> 0.231 78.8
SiC (mp-11714) <0 0 1> <1 0 1> 0.232 171.1
Au (mp-81) <1 0 0> <0 0 1> 0.238 141.9
C (mp-48) <0 0 1> <1 1 0> 0.261 168.7
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.261 56.2
BN (mp-984) <1 0 1> <0 0 1> 0.274 205.0
Al (mp-134) <1 1 1> <1 1 0> 0.277 56.2
CsI (mp-614603) <1 0 0> <0 0 1> 0.279 63.1
CdSe (mp-2691) <1 0 0> <0 0 1> 0.282 78.8
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.283 283.8
MgO (mp-1265) <1 0 0> <0 0 1> 0.298 141.9
Ag (mp-124) <1 1 1> <1 0 0> 0.308 119.3
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.311 299.5
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.314 56.2
CdS (mp-672) <1 1 1> <0 0 1> 0.316 205.0
C (mp-66) <1 1 0> <1 0 1> 0.319 213.9
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.324 157.7
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.326 315.4
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.328 116.8
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.335 213.9
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.339 278.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
210 54 79 0 0 0
54 210 79 0 0 0
79 79 209 0 0 0
0 0 0 88 0 0
0 0 0 0 88 0
0 0 0 0 0 64
Compliance Tensor Sij (10-12Pa-1)
5.6 -0.8 -1.8 0 0 0
-0.8 5.6 -1.8 0 0 0
-1.8 -1.8 6.2 0 0 0
0 0 0 11.3 0 0
0 0 0 0 11.3 0
0 0 0 0 0 15.7
Shear Modulus GV
76 GPa
Bulk Modulus KV
117 GPa
Shear Modulus GR
74 GPa
Bulk Modulus KR
117 GPa
Shear Modulus GVRH
75 GPa
Bulk Modulus KVRH
117 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Dy(CuSi)2 (mp-2917) 0.0111 0.000 3
Gd(CuSi)2 (mp-1097761) 0.0231 0.000 3
Tb(CuSi)2 (mp-3456) 0.0185 0.000 3
Pu(CuSi)2 (mp-20751) 0.0278 0.230 3
Pu(SiRh)2 (mp-22657) 0.0198 0.082 3
La3Cu4(P2O)2 (mp-6309) 0.5835 0.000 4
SrIn4 (mp-22466) 0.1526 0.010 2
YbGa4 (mp-1088) 0.1596 0.000 2
CaGa4 (mp-1976) 0.1521 0.000 2
SrAl4 (mp-2775) 0.0717 0.000 2
BaAl4 (mp-1903) 0.0564 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cu_pv Si
Final Energy/Atom
-5.7000 eV
Corrected Energy
-28.3578 eV
Uncorrected energy = -28.4998 eV Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV Corrected energy = -28.3578 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 629221
  • 164066
  • 23551
Submitted by
User remarks:
  • Copper yttrium silicide (2/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)