Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.752 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAl2NiO4 |
Band Gap3.065 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 297.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 139.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 287.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 161.4 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 297.7 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 198.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 99.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 172.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 139.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 161.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 139.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 57.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 198.4 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 297.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 139.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 287.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 57.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 297.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 99.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 99.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 57.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 172.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 115.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 172.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 57.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 115.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 172.5 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 287.5 |
Al (mp-134) | <1 0 0> | <1 0 1> | 99.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 115.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 57.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 99.2 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 287.5 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 230.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 230.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 297.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 150.8 |
C (mp-66) | <1 1 0> | <1 0 1> | 198.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 1> | 198.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 115.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 172.5 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 297.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 161.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 139.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 57.5 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 297.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2NiO4 (mp-699371) | 0.0178 | 0.005 | 3 |
Al2NiO4 (mp-698649) | 0.0303 | 0.004 | 3 |
Al2NiO4 (mp-705646) | 0.0714 | 0.010 | 3 |
Al2NiO4 (mp-705610) | 0.0713 | 0.009 | 3 |
Al2NiO4 (mvc-16266) | 0.0090 | 0.006 | 3 |
Li5Mn2Fe17O32 (mp-777733) | 0.1217 | 0.070 | 4 |
Li5Fe7O3F13 (mp-851009) | 0.1559 | 0.053 | 4 |
Li3Fe3OF7 (mp-764593) | 0.1521 | 0.045 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.1248 | 0.067 | 4 |
Li5Co7O3F13 (mp-849472) | 0.1625 | 0.053 | 4 |
Fe3O4 (mp-715491) | 0.1716 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.2001 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.1560 | 0.057 | 2 |
Fe3O4 (mp-31770) | 0.1860 | 0.015 | 2 |
Fe3O4 (mp-716052) | 0.2116 | 0.073 | 2 |
Li4Co3Ni3(TeO8)2 (mp-762071) | 0.2285 | 0.036 | 5 |
Li4Cr3Ni3(TeO8)2 (mp-761407) | 0.2159 | 0.007 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.2236 | 0.009 | 5 |
TaTi9Al3Zn23O48 (mp-686614) | 0.2163 | 0.054 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.1957 | 0.053 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6603 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6461 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6552 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6580 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6593 | 0.661 | 6 |
Explore more synthesis descriptions for materials of composition Al2NiO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Al Ni_pv O |
Final Energy/Atom-6.7648 eV |
Corrected Energy-313.9585 eV
-313.9585 eV = -284.1195 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 12.9840 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)