material

FeSiRu2

ID:

mp-3464

DOI:

10.17188/1206862


Tags: High pressure experimental phase Iron ruthenium silicon (1/2/1) Iron ruthenium silicide (1/2/1)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.359 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.18 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaF3 (mp-905) <0 0 1> <1 1 1> 0.000 181.9
GaN (mp-804) <0 0 1> <1 1 1> 0.007 242.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.008 315.0
Cu (mp-30) <1 1 0> <1 1 0> 0.013 148.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.014 280.0
Ni (mp-23) <1 1 0> <1 1 0> 0.015 297.0
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.017 60.6
GaN (mp-804) <1 0 1> <1 0 0> 0.018 210.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.022 175.0
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.023 280.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.025 297.0
Au (mp-81) <1 0 0> <1 0 0> 0.035 35.0
Au (mp-81) <1 1 0> <1 1 0> 0.035 49.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.037 175.0
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.057 315.0
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.059 175.0
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.072 175.0
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.091 303.1
Al (mp-134) <1 0 0> <1 0 0> 0.099 280.0
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.113 148.5
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.114 181.9
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.116 315.0
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.121 60.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.126 175.0
Ag (mp-124) <1 0 0> <1 0 0> 0.128 35.0
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.128 346.5
Ag (mp-124) <1 1 0> <1 1 0> 0.128 49.5
GaSe (mp-1943) <0 0 1> <1 1 1> 0.134 242.5
CdS (mp-672) <0 0 1> <1 1 1> 0.140 60.6
AlN (mp-661) <1 1 1> <1 1 0> 0.140 198.0
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.154 148.5
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.158 315.0
AlN (mp-661) <1 0 1> <1 1 0> 0.161 247.5
GaTe (mp-542812) <1 0 0> <1 1 1> 0.164 181.9
LiF (mp-1138) <1 0 0> <1 0 0> 0.170 280.0
WS2 (mp-224) <0 0 1> <1 1 0> 0.193 247.5
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.193 247.5
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.200 280.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.201 175.0
InP (mp-20351) <1 0 0> <1 0 0> 0.211 35.0
InP (mp-20351) <1 1 0> <1 1 0> 0.212 49.5
ZnO (mp-2133) <1 0 0> <1 1 0> 0.212 346.5
InP (mp-20351) <1 1 1> <1 1 1> 0.214 60.6
AlN (mp-661) <1 1 0> <1 1 0> 0.215 297.0
TePb (mp-19717) <1 0 0> <1 0 0> 0.229 175.0
Mg (mp-153) <0 0 1> <1 1 0> 0.232 247.5
Mg (mp-153) <1 0 1> <1 0 0> 0.239 210.0
PbSe (mp-2201) <1 0 0> <1 0 0> 0.254 315.0
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.272 140.0
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.273 245.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
381 165 165 0 0 0
165 381 165 0 0 0
165 165 381 0 0 0
0 0 0 122 0 0
0 0 0 0 122 0
0 0 0 0 0 122
Compliance Tensor Sij (10-12Pa-1)
3.6 -1.1 -1.1 0 0 0
-1.1 3.6 -1.1 0 0 0
-1.1 -1.1 3.6 0 0 0
0 0 0 8.2 0 0
0 0 0 0 8.2 0
0 0 0 0 0 8.2
Shear Modulus GV
116 GPa
Bulk Modulus KV
237 GPa
Shear Modulus GR
116 GPa
Bulk Modulus KR
237 GPa
Shear Modulus GVRH
116 GPa
Bulk Modulus KVRH
237 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiFeCoSi (mp-998971) 0.0000 0.027 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSbPd (mp-10179) 0.0000 0.067 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
TiGaFeCo (mp-998964) 0.0000 0.000 4
Na3As (mp-8860) 0.0000 0.045 2
TbMg3 (mp-7381) 0.0000 0.000 2
Li3Tl (mp-7396) 0.0000 0.000 2
LiGa (mp-1307) 0.0000 0.000 2
Sr3In (mp-31349) 0.0000 0.125 2
ZrNi2Sn (mp-19877) 0.0000 0.048 3
AlVFe2 (mp-5778) 0.0000 0.000 3
AlCrNi2 (mp-10885) 0.0000 0.131 3
GaFeCo2 (mp-30551) 0.0000 0.000 3
ZrAlCo2 (mp-3909) 0.0000 0.000 3
Lu (mp-10190) 0.0000 0.136 1
Dy (mp-10751) 0.0000 0.139 1
La (mp-10023) 0.0000 0.143 1
Rb (mp-70) 0.0000 0.000 1
Cs (mp-1) 0.0000 0.002 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Fe_pv Ru_pv
Final Energy/Atom
-8.4686 eV
Corrected Energy
-33.8744 eV
-33.8744 eV = -33.8744 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 633246
  • 53525
  • 633245
Submitted by
User remarks:
  • High pressure experimental phase
  • Iron ruthenium silicon (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)