material

BaNbS3

ID:

mp-35143

DOI:

10.17188/1206939


Tags: Barium niobium sulfide (1/1/3)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.843 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ba8Nb7S24 + Nb3S5 + BaS
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 659538 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 1> <0 0 1> 0.000 125.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.000 167.4
WS2 (mp-224) <0 0 1> <0 0 1> 0.000 167.4
Mg (mp-153) <0 0 1> <0 0 1> 0.006 167.4
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.007 125.6
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.008 125.6
DyScO3 (mp-31120) <1 0 1> <1 1 0> 0.009 276.9
Cu (mp-30) <1 1 1> <0 0 1> 0.010 293.0
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.011 138.5
NaCl (mp-22862) <1 1 1> <0 0 1> 0.011 167.4
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.014 138.5
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.014 231.5
CdS (mp-672) <0 0 1> <0 0 1> 0.016 293.0
Ge (mp-32) <1 0 0> <1 0 0> 0.018 199.8
LiF (mp-1138) <1 0 0> <1 0 0> 0.023 199.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.023 125.6
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.024 125.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.025 159.9
GaAs (mp-2534) <1 0 0> <1 0 0> 0.031 199.8
TbScO3 (mp-31119) <1 0 1> <1 1 0> 0.033 276.9
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.043 138.5
Ni (mp-23) <1 1 0> <1 0 1> 0.045 173.6
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.048 199.8
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.049 334.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.049 359.7
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.052 319.8
Al (mp-134) <1 1 0> <1 1 0> 0.053 69.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.061 167.4
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.061 159.9
MgO (mp-1265) <1 0 0> <0 0 1> 0.062 293.0
SiC (mp-7631) <1 0 0> <1 0 0> 0.066 279.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.071 279.8
KCl (mp-23193) <1 0 0> <1 0 1> 0.071 289.4
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.073 293.0
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.073 138.5
SiC (mp-11714) <0 0 1> <1 0 0> 0.073 279.8
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.074 69.2
CdWO4 (mp-19387) <0 0 1> <1 1 1> 0.075 242.7
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.075 334.9
SiC (mp-7631) <0 0 1> <1 0 0> 0.078 279.8
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.079 279.8
ZnO (mp-2133) <0 0 1> <1 1 0> 0.084 207.7
BN (mp-984) <0 0 1> <1 0 0> 0.088 199.8
MgF2 (mp-1249) <1 1 1> <1 1 1> 0.089 242.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.096 138.5
NaCl (mp-22862) <1 1 0> <1 1 0> 0.101 138.5
Mg (mp-153) <1 0 1> <0 0 1> 0.102 209.3
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.103 207.7
ZnO (mp-2133) <1 0 1> <0 0 1> 0.110 293.0
GaN (mp-804) <0 0 1> <0 0 1> 0.110 167.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
74 32 21 0 0 0
32 74 21 0 0 0
21 21 142 0 0 0
0 0 0 2 0 0
0 0 0 0 2 0
0 0 0 0 0 21
Compliance Tensor Sij (10-12Pa-1)
16.8 -6.9 -1.5 0 0 0
-6.9 16.8 -1.5 0 0 0
-1.5 -1.5 7.5 0 0 0
0 0 0 405.4 0 0
0 0 0 0 405.4 0
0 0 0 0 0 47.5
Shear Modulus GV
20 GPa
Bulk Modulus KV
49 GPa
Shear Modulus GR
5 GPa
Bulk Modulus KR
46 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
13.23
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BaTaS3 (mp-4001) 0.0573 0.000 3
CsScCl3 (mp-27359) 0.2026 0.019 3
BaTaSe3 (mp-1078588) 0.1472 0.026 3
BaTiSe3 (mp-1079893) 0.2565 0.000 3
CsTiBr3 (mp-22962) 0.2028 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Nb_pv S
Final Energy/Atom
-6.3312 eV
Corrected Energy
-67.2930 eV
-67.2930 eV = -63.3123 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 659538
User remarks:
  • Ordering of Disordered Crystal

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)