material

MgCuSb

ID:

mp-3522

DOI:

10.17188/1206961


Tags: Copper(I) magnesium antimonide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.242 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 77364 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <1 0 0> 0.000 155.8
Ag (mp-124) <1 1 0> <1 1 0> 0.000 220.3
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.000 194.7
Ni (mp-23) <1 1 0> <1 1 0> 0.000 330.5
LiF (mp-1138) <1 1 1> <1 1 1> 0.001 202.4
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.001 220.3
GaSe (mp-1943) <0 0 1> <1 1 1> 0.002 202.4
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.004 311.6
CdTe (mp-406) <1 0 0> <1 0 0> 0.004 350.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.009 350.5
PbSe (mp-2201) <1 0 0> <1 0 0> 0.010 38.9
PbSe (mp-2201) <1 1 0> <1 1 0> 0.010 55.1
PbSe (mp-2201) <1 1 1> <1 1 1> 0.010 67.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.012 155.8
Au (mp-81) <1 0 0> <1 0 0> 0.013 155.8
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.014 67.5
Au (mp-81) <1 1 0> <1 1 0> 0.014 220.3
Au (mp-81) <1 1 1> <1 1 1> 0.014 269.8
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.014 67.5
GaSb (mp-1156) <1 0 0> <1 0 0> 0.023 38.9
GaSb (mp-1156) <1 1 0> <1 1 0> 0.024 55.1
GaSb (mp-1156) <1 1 1> <1 1 1> 0.025 67.5
Cu (mp-30) <1 1 0> <1 1 0> 0.028 55.1
Cu (mp-30) <1 1 1> <1 1 1> 0.029 67.5
Cu (mp-30) <1 0 0> <1 1 0> 0.030 275.4
AlN (mp-661) <0 0 1> <1 0 0> 0.032 272.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.037 116.8
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.037 202.4
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.037 165.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.038 311.6
Mg (mp-153) <0 0 1> <1 1 1> 0.038 269.8
CdSe (mp-2691) <1 0 0> <1 0 0> 0.039 38.9
CdSe (mp-2691) <1 1 0> <1 1 0> 0.040 55.1
CdSe (mp-2691) <1 1 1> <1 1 1> 0.041 67.5
GaN (mp-804) <0 0 1> <1 0 0> 0.046 311.6
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.049 269.8
ZnO (mp-2133) <1 0 1> <1 1 0> 0.054 275.4
ZnO (mp-2133) <1 1 0> <1 1 0> 0.055 330.5
MgO (mp-1265) <1 0 0> <1 0 0> 0.064 311.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.069 311.6
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.070 311.6
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.078 155.8
Te2Mo (mp-602) <1 0 0> <1 1 1> 0.079 269.8
Te2W (mp-22693) <0 1 0> <1 1 1> 0.084 269.8
ZnO (mp-2133) <1 1 1> <1 1 0> 0.085 220.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.091 38.9
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.095 55.1
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.096 67.5
SiC (mp-11714) <0 0 1> <1 1 0> 0.097 165.2
SiC (mp-7631) <0 0 1> <1 1 0> 0.100 165.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
107 48 48 0 0 0
48 107 48 0 0 0
48 48 107 0 0 0
0 0 0 42 0 0
0 0 0 0 42 0
0 0 0 0 0 42
Compliance Tensor Sij (10-12Pa-1)
12.9 -4 -4 0 0 0
-4 12.9 -4 0 0 0
-4 -4 12.9 0 0 0
0 0 0 23.6 0 0
0 0 0 0 23.6 0
0 0 0 0 0 23.6
Shear Modulus GV
37 GPa
Bulk Modulus KV
68 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
68 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
0.15
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MnNiSb (mp-22541) 0.0000 0.321 3
HoSnAu (mp-30390) 0.0000 0.000 3
ScNiBi (mp-30459) 0.0000 0.000 3
HfSbRu (mp-31456) 0.0000 0.030 3
HfSnPt (mp-20889) 0.0000 0.489 3
Rb2S (mp-8041) 0.0000 0.000 2
AcH2 (mp-24147) 0.0000 0.000 2
Mg2Ge (mp-408) 0.0000 0.000 2
PbF2 (mp-315) 0.0000 0.000 2
CaF2 (mp-2741) 0.0000 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Cu_pv Sb
Final Energy/Atom
-3.5171 eV
Corrected Energy
-10.7434 eV
Uncorrected energy = -10.5514 eV Composition-based energy adjustment (-0.192 eV/atom x 1.0 atoms) = -0.1920 eV Corrected energy = -10.7434 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 77364
  • 412294
Submitted by
User remarks:
  • Copper(I) magnesium antimonide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)