material

Ag2O

ID:

mp-353

DOI:

10.17188/1206976


Tags: Silver oxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.323 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.78 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.060 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pn3m [224]
Hall
P 4n 2 3 1n
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 31058 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <1 1 1> <1 0 0> -0.002 210.9
KTaO3 (mp-3614) <1 1 1> <1 0 0> -0.001 140.6
ZnO (mp-2133) <0 0 1> <1 1 1> 0.000 121.8
C (mp-66) <1 1 0> <1 1 0> 0.000 198.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.000 298.3
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.000 324.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.001 210.9
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.001 284.1
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.002 210.9
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.002 281.2
WS2 (mp-224) <0 0 1> <1 1 0> 0.002 132.6
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.002 132.6
Ga2O3 (mp-886) <0 1 0> <1 1 1> 0.002 284.1
KCl (mp-23193) <1 1 1> <1 1 1> 0.003 284.1
CdS (mp-672) <1 1 0> <1 1 0> 0.003 99.4
C (mp-48) <1 0 0> <1 1 0> 0.005 232.0
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.006 132.6
ZnO (mp-2133) <1 0 0> <1 1 0> 0.007 298.3
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.008 351.5
Cu (mp-30) <1 0 0> <1 0 0> 0.008 117.2
WS2 (mp-224) <1 0 1> <1 1 0> 0.009 232.0
Al (mp-134) <1 1 1> <1 0 0> 0.010 140.6
Al (mp-134) <1 0 0> <1 0 0> 0.012 210.9
AlN (mp-661) <1 0 0> <1 1 0> 0.013 298.3
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.013 210.9
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.015 281.2
Mg (mp-153) <0 0 1> <1 1 0> 0.017 132.6
C (mp-48) <0 0 1> <1 1 1> 0.018 162.4
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.018 281.2
Te2W (mp-22693) <0 1 1> <1 0 0> 0.023 117.2
GaN (mp-804) <1 0 1> <1 1 1> 0.024 284.1
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.026 232.0
AlN (mp-661) <0 0 1> <1 1 1> 0.026 162.4
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.026 265.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.027 364.5
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.030 351.5
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.030 187.5
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.033 265.1
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.033 210.9
GaN (mp-804) <1 1 0> <1 1 0> 0.033 265.1
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.035 351.5
InP (mp-20351) <1 1 0> <1 1 0> 0.036 99.4
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.038 304.6
Au (mp-81) <1 1 0> <1 1 0> 0.040 99.4
Au (mp-81) <1 1 1> <1 1 1> 0.040 121.8
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.041 210.9
LiNbO3 (mp-3731) <1 0 0> <1 1 0> 0.042 298.3
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.043 265.1
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.045 351.5
CdS (mp-672) <1 1 1> <1 0 0> 0.045 210.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
68 68 68 0 0 0
68 68 68 0 0 0
68 68 68 0 0 0
0 0 0 1 0 0
0 0 0 0 1 0
0 0 0 0 0 1
Compliance Tensor Sij (10-12Pa-1)
-1295.5 650.2 650.2 0 0 0
650.2 -1295.5 650.2 0 0 0
650.2 650.2 -1295.5 0 0 0
0 0 0 856.4 0 0
0 0 0 0 856.4 0
0 0 0 0 0 856.4
Shear Modulus GV
1 GPa
Bulk Modulus KV
68 GPa
Shear Modulus GR
-1 GPa
Bulk Modulus KR
68 GPa
Shear Modulus GVRH
-0 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
-8.12
Poisson's Ratio
0.50

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.75 0.00 0.00
0.00 6.75 0.00
0.00 0.00 6.75
Dielectric Tensor εij (total)
7.35 0.00 0.00
0.00 7.35 0.00
0.00 0.00 7.35
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.75
Polycrystalline dielectric constant εpoly
(total)
7.35
Refractive Index n
2.60
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ag3AuS2 (mp-34460) 0.4518 0.000 3
Be(CN)2 (mp-35687) 0.7135 0.226 3
AlPO4 (mp-545974) 0.4537 0.011 3
Mg2ZnN2 (mp-1029265) 0.7128 1.954 3
ZnSO4 (mp-545756) 0.6996 0.038 3
CuCSN (mp-672285) 0.7330 0.162 4
CuCSN (mp-559044) 0.7279 0.162 4
PtO2 (mp-20119) 0.0000 0.794 2
Cs2Se (mp-1011697) 0.0000 0.306 2
Pd2O (mp-10729) 0.0000 0.140 2
CdB2 (mp-1072852) 0.0000 2.573 2
Zr2O (mp-10735) 0.0000 0.228 2
C (mp-1095534) 0.6917 1.121 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

A series of silver phosphate samples with composition described by a nominal formula xAgI(100-x) (0.75Ag2O0.25P2O5), where 50x85, were prepared by a standard melt-quenching technique [1]. The [...]
The silver iodate(VII), Ag5IO6, was obtained by reacting a stoichiometric mixture of Ag2O and KIO3, at elevated oxygen pressure, adding a small portion of distilled water. The synthesis was done at 67 [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Ag2O.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ag O
Final Energy/Atom
-3.6312 eV
Corrected Energy
-23.1615 eV
Uncorrected energy = -21.7875 eV Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV Corrected energy = -23.1615 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 174090
  • 174091
  • 174089
  • 174088
  • 247821
  • 31058
  • 605623
  • 174087
  • 173984
  • 281041
  • 174092
  • 35540
  • 246904
Submitted by
User remarks:
  • Silver oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)