Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.923 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.906 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421m [113] |
HallP 4 2ab |
Point Group42m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 335.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 254.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 287.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 169.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 254.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 271.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 335.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 335.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 139.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 203.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 305.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 144.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 183.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 135.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 287.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 305.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 339.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 335.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 305.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 254.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 271.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 254.4 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 305.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 254.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 339.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 279.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 61.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 237.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 101.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 209.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 305.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 254.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 139.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 203.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 237.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 67.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 191.9 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 254.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 135.7 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 191.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 244.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 209.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 50.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 135.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 305.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 271.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 152.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 339.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 209.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.12781 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.12781 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.73790 |
Piezoelectric Modulus ‖eij‖max0.19120 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
1.00000 |
1.00000 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tc2P3 (mp-9895) | 0.6584 | 0.000 | 2 |
Tc2P3 (mp-11690) | 0.6205 | 0.005 | 2 |
Tc2As3 (mp-8886) | 0.7446 | 0.000 | 2 |
Ge3Pt2 (mp-571640) | 0.6640 | 0.000 | 2 |
ErAgTe2 (mp-12902) | 0.0366 | 0.000 | 3 |
YAgTe2 (mp-12903) | 0.0482 | 0.000 | 3 |
HoAgSe2 (mp-12955) | 0.5890 | 0.000 | 3 |
HoAgTe2 (mp-12904) | 0.0248 | 0.000 | 3 |
DyAgTe2 (mp-4024) | 0.0112 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points24 |
U Values-- |
PseudopotentialsVASP PAW: Ag Te Tb_3 |
Final Energy/Atom-4.3587 eV |
Corrected Energy-34.8700 eV
-34.8700 eV = -34.8700 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)