Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.200 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToDyAgS2 + Dy2S3 |
Band Gap1.837 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 277.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 208.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 277.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 240.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 278.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 277.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.3 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 98.3 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 120.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 120.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 294.8 |
Al (mp-134) | <1 0 0> | <1 0 1> | 98.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 208.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 138.6 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 196.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 294.8 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 278.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 98.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 120.5 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 277.3 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 69.3 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 98.3 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 1 1> | 120.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 277.3 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 277.3 |
Cu (mp-30) | <1 0 0> | <1 0 1> | 196.6 |
Cu (mp-30) | <1 1 0> | <1 0 1> | 294.8 |
C (mp-66) | <1 1 0> | <1 0 1> | 196.6 |
GaTe (mp-542812) | <0 0 1> | <1 0 1> | 294.8 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 69.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 278.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 208.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 277.3 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 138.6 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 277.3 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 277.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.3 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 98.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 277.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.3 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 98.3 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 294.8 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 209.0 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 196.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 1> | 240.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 277.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 1> | 294.8 |
Si (mp-149) | <1 0 0> | <0 0 1> | 277.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd5AgSe8 (mp-685977) | 0.1260 | 0.025 | 3 |
Nd5AgS8 (mp-37449) | 0.1302 | 0.021 | 3 |
Sm5AgS8 (mp-37923) | 0.0879 | 0.022 | 3 |
Gd5AgS8 (mp-676156) | 0.1110 | 0.394 | 3 |
Tb5AgS8 (mp-33449) | 0.0612 | 0.030 | 3 |
Pr4Ge3 (mp-570606) | 0.3878 | 0.000 | 2 |
Hf3N4 (mp-11660) | 0.3971 | 0.069 | 2 |
Pr4As3 (mp-2365) | 0.3925 | 0.020 | 2 |
Eu4As3 (mp-20995) | 0.4089 | 0.000 | 2 |
Ba3P2 (mp-32606) | 0.3702 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Ag S |
Final Energy/Atom-6.0320 eV |
Corrected Energy-89.7561 eV
-89.7561 eV = -84.4484 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)