material

HfGaCo2

ID:

mp-3576

DOI:

10.17188/1207070


Tags: Cobalt gallium hafnium (2/1/1)

Material Details

Final Magnetic Moment
1.015 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.482 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.09 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <1 0 0> 0.000 327.3
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.001 72.7
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.001 102.8
ZnO (mp-2133) <1 0 1> <1 0 0> 0.002 218.2
NaCl (mp-22862) <1 0 0> <1 0 0> 0.004 290.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.010 36.4
MgO (mp-1265) <1 1 0> <1 1 0> 0.011 51.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.013 72.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.015 251.9
GaN (mp-804) <0 0 1> <1 1 1> 0.016 63.0
C (mp-66) <1 1 0> <1 1 0> 0.017 308.5
C (mp-48) <0 0 1> <1 1 1> 0.018 63.0
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.024 145.5
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.025 205.7
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.025 251.9
SiC (mp-7631) <0 0 1> <1 0 0> 0.039 290.9
SiC (mp-11714) <0 0 1> <1 0 0> 0.041 290.9
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.056 154.3
Ni (mp-23) <1 0 0> <1 1 0> 0.063 257.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.066 36.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.067 145.5
PbS (mp-21276) <1 1 0> <1 1 0> 0.069 51.4
PbS (mp-21276) <1 1 1> <1 1 1> 0.069 63.0
Al (mp-134) <1 0 0> <1 0 0> 0.074 145.5
Al (mp-134) <1 1 0> <1 1 0> 0.076 205.7
Al (mp-134) <1 1 1> <1 1 1> 0.077 251.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.095 308.5
Cu (mp-30) <1 1 0> <1 1 0> 0.103 205.7
Ag (mp-124) <1 0 0> <1 0 0> 0.112 290.9
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.113 154.3
ZnO (mp-2133) <1 0 0> <1 1 1> 0.130 314.9
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.131 218.2
MgO (mp-1265) <1 1 1> <1 0 0> 0.182 254.5
Ni (mp-23) <1 1 0> <1 1 0> 0.203 51.4
Ni (mp-23) <1 1 1> <1 1 1> 0.205 63.0
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.223 363.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.280 290.9
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.292 154.3
Mg (mp-153) <1 0 0> <1 0 0> 0.301 181.8
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.318 254.5
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.322 327.3
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.334 205.7
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.339 290.9
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.345 290.9
YAlO3 (mp-3792) <1 0 0> <1 1 1> 0.353 314.9
C (mp-48) <1 0 1> <1 0 0> 0.363 218.2
C (mp-48) <1 1 0> <1 0 0> 0.386 327.3
Au (mp-81) <1 1 1> <1 0 0> 0.392 181.8
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.404 188.9
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.404 314.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
253 135 135 0 0 0
135 253 135 0 0 0
135 135 253 0 0 0
0 0 0 92 0 0
0 0 0 0 92 0
0 0 0 0 0 92
Compliance Tensor Sij (10-12Pa-1)
6.3 -2.2 -2.2 0 0 0
-2.2 6.3 -2.2 0 0 0
-2.2 -2.2 6.3 0 0 0
0 0 0 10.9 0 0
0 0 0 0 10.9 0
0 0 0 0 0 10.9
Shear Modulus GV
79 GPa
Bulk Modulus KV
174 GPa
Shear Modulus GR
75 GPa
Bulk Modulus KR
174 GPa
Shear Modulus GVRH
77 GPa
Bulk Modulus KVRH
174 GPa
Elastic Anisotropy
0.23
Poisson's Ratio
0.31

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
60
U Values
--
Pseudopotentials
VASP PAW: Co Ga_d Hf_pv
Final Energy/Atom
-7.2834 eV
Corrected Energy
-29.1337 eV
-29.1337 eV = -29.1337 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 623080
  • 102433

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)