material

Y2CdS4

ID:

mp-35785

DOI:

10.17188/1207073


Tags: Cadmium yttrium sulfide (1/2/4)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.049 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.84 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.347 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 620370 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 128.0
C (mp-66) <1 0 0> <1 0 0> 0.002 128.0
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.007 128.0
ZnO (mp-2133) <1 1 0> <1 1 0> 0.023 181.0
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.033 128.0
TePb (mp-19717) <1 1 0> <1 1 0> 0.062 181.0
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.081 128.0
NaCl (mp-22862) <1 0 0> <1 0 0> 0.082 128.0
NaCl (mp-22862) <1 1 0> <1 1 0> 0.085 181.0
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.107 128.0
ZnO (mp-2133) <1 1 1> <1 0 0> 0.139 128.0
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.156 181.0
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.191 256.0
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.225 256.0
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.238 181.0
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.257 256.0
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.280 128.0
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.330 181.0
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.404 128.0
CdTe (mp-406) <1 1 0> <1 1 0> 0.504 181.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.659 128.0
CsI (mp-614603) <1 1 0> <1 1 0> 0.689 181.0
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 1.002 128.0
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 1.048 181.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
82 51 51 0 0 0
51 82 51 0 0 0
51 51 82 0 0 0
0 0 0 28 0 0
0 0 0 0 28 0
0 0 0 0 0 28
Compliance Tensor Sij (10-12Pa-1)
23.2 -8.9 -8.9 0 0 0
-8.9 23.2 -8.9 0 0 0
-8.9 -8.9 23.2 0 0 0
0 0 0 35.2 0 0
0 0 0 0 35.2 0
0 0 0 0 0 35.2
Shear Modulus GV
23 GPa
Bulk Modulus KV
62 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
62 GPa
Elastic Anisotropy
0.45
Poisson's Ratio
0.34

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.14 -0.00 -0.00
-0.00 6.14 0.00
-0.00 0.00 6.14
Dielectric Tensor εij (total)
14.67 -0.00 -0.00
-0.00 14.67 0.00
-0.00 0.00 14.67
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.14
Polycrystalline dielectric constant εpoly
(total)
14.67
Refractive Index n
2.48
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mg(InS2)2 (mp-20493) 0.0088 0.004 3
Mg(InSe2)2 (mp-1001034) 0.0080 0.027 3
Dy2CdS4 (mp-16267) 0.0044 0.000 3
Cr2CuTe4 (mp-22625) 0.0087 0.000 3
Ho2CdSe4 (mp-4284) 0.0028 0.011 3
Cr4FeCuS8 (mp-6685) 0.1225 0.000 4
Li2V3CrO8 (mp-853131) 0.1577 0.032 4
Li2NbV3O8 (mp-774016) 0.1753 0.006 4
Li2V3CoO8 (mp-765546) 0.1777 0.223 4
Li2VFe3O8 (mp-771748) 0.1834 0.079 4
Co3S4 (mp-943) 0.0082 0.000 2
Co3Se4 (mp-20456) 0.0062 0.000 2
Hf3N4 (mp-755988) 0.0187 0.016 2
Zr3N4 (mp-754381) 0.0170 0.035 2
Si3N4 (mp-2075) 0.0052 0.147 2
Li14Mn22Cr3Cu3O56 (mp-735790) 0.3607 0.014 5
Li4Cr3Fe3(TeO8)2 (mp-773518) 0.3661 0.054 5
Li4Mn3Cr3(CuO8)2 (mp-765456) 0.3482 0.069 5
Li4Cr3Cu3(SbO8)2 (mp-783908) 0.3677 0.035 5
Li4Cr3Fe3(SbO8)2 (mp-771925) 0.3542 6.495 5
Li3MnFeCo(PO4)3 (mp-764931) 0.7449 0.017 6
Li3MnFeCo(PO4)3 (mp-764809) 0.7369 0.014 6
Li3MnFeCo(PO4)3 (mp-764869) 0.7412 0.032 6
Li3MnFeCo(PO4)3 (mp-764707) 0.7439 0.035 6
Li3MnFeCo(PO4)3 (mp-764969) 0.7350 0.057 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cd S
Final Energy/Atom
-6.0102 eV
Corrected Energy
-89.4508 eV
-89.4508 eV = -84.1431 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 620371
  • 620370
User remarks:
  • Ordering of Disordered Crystal

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)