Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.675 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2Bi8Se13 + K3BiSe3 |
Band Gap1.092 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 238.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 190.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 305.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 38.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 190.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 238.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 88.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 343.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 88.2 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 190.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 152.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 305.1 |
BN (mp-984) | <1 1 0> | <1 0 1> | 264.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 152.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 238.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 343.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 112.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 190.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 264.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 317.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 317.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 237.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 266.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 343.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 305.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 38.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 159.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 305.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 317.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 190.7 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 190.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 238.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 190.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 266.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 266.9 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 264.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 317.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 305.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 305.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 228.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 343.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 305.1 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 264.5 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 190.7 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 190.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 264.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 76.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaAsSe2 (mp-34663) | 0.1182 | 0.115 | 3 |
NaYbO2 (mp-756878) | 0.1010 | 0.098 | 3 |
LiNiO2 (mp-770635) | 0.0393 | 0.015 | 3 |
Ca2NF (mp-33588) | 0.0920 | 0.030 | 3 |
TlBiS2 (mp-36946) | 0.0931 | 0.120 | 3 |
Li2CoCuO4 (mp-775052) | 0.0281 | 0.090 | 4 |
Li2NiSnO4 (mp-773418) | 0.1722 | 0.013 | 4 |
Li2MnCrO4 (mp-773308) | 0.1736 | 0.035 | 4 |
Li2CrNiO4 (mp-773255) | 0.1447 | 0.073 | 4 |
Li2CuNiO4 (mp-849680) | 0.1307 | 0.015 | 4 |
Te2Au (mp-1662) | 0.5104 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3824 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.4989 | 0.009 | 2 |
VN (mvc-13303) | 0.6079 | 0.183 | 2 |
Te2Au (mp-567525) | 0.4651 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5794 | 0.005 | 5 |
Sb (mp-632286) | 0.6311 | 0.059 | 1 |
Bi (mp-567379) | 0.6912 | 0.062 | 1 |
Te (mp-570459) | 0.5812 | 0.044 | 1 |
Te (mp-105) | 0.7106 | 0.047 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Bi Se |
Final Energy/Atom-3.6733 eV |
Corrected Energy-29.3868 eV
-29.3868 eV = -29.3868 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)