Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.267 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg2S + AgBr |
Band Gap0.509 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFmm2 [42] |
HallF 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 94.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 194.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 282.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 282.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 194.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 136.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 282.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 282.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 282.6 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 282.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 190.7 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 292.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 190.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 282.6 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 188.4 |
C (mp-66) | <1 1 0> | <0 1 0> | 286.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 194.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 282.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 292.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 292.2 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 282.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 282.6 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 97.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 286.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 188.4 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 194.8 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 194.8 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 134.0 |
NaCl (mp-22862) | <1 1 0> | <0 1 1> | 134.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 282.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 94.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 282.6 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 188.4 |
MgF2 (mp-1249) | <0 0 1> | <0 1 1> | 134.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 292.2 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 194.8 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 1> | 134.0 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 194.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag3SI (mp-673825) | 0.2753 | 0.073 | 3 |
GaBiO3 (mp-755568) | 0.5755 | 0.051 | 3 |
CrBiO3 (mp-557515) | 0.5127 | 0.015 | 3 |
FeBiO3 (mp-601706) | 0.4838 | 0.062 | 3 |
AlBiO3 (mp-551918) | 0.5665 | 0.053 | 3 |
NaTi2BiO6 (mp-39681) | 0.6286 | 0.014 | 4 |
LaTaN2O (mp-550514) | 0.6151 | 0.000 | 4 |
NaNbO2F (mp-557590) | 0.6512 | 0.180 | 4 |
CrFe(BiO3)2 (mp-559001) | 0.5031 | 0.016 | 4 |
TiFe(BiO3)2 (mp-604652) | 0.4928 | 0.015 | 4 |
SrLaFeRuO6 (mp-697833) | 0.6480 | 0.032 | 5 |
SrCoBiRuO6 (mp-743579) | 0.5905 | 0.086 | 5 |
Ca3La7Ti5Cr5O30 (mp-744126) | 0.6349 | 0.042 | 5 |
Ca3La5Mn7CrO24 (mp-743745) | 0.6449 | 0.135 | 5 |
CaLaVFeO6 (mp-705523) | 0.6048 | 0.287 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag S Br |
Final Energy/Atom-2.9888 eV |
Corrected Energy-31.2149 eV
-31.2149 eV = -29.8880 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)