Final Magnetic Moment0.429 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.047 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSm5Sb3 + SmSb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.0 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 250.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 153.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 125.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 153.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 250.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 265.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 250.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 265.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 88.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 125.0 |
BN (mp-984) | <0 0 1> | <1 1 1> | 153.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 153.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 250.0 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 250.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 250.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 88.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 125.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 88.4 |
C (mp-66) | <1 1 1> | <1 1 1> | 153.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 250.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.8 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 125.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 176.8 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 125.0 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 153.1 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 88.4 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 125.0 |
Si (mp-149) | <1 1 0> | <1 1 0> | 125.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 88.4 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 265.1 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 153.1 |
Si (mp-149) | <1 1 1> | <1 1 1> | 153.1 |
C (mp-48) | <1 0 0> | <1 1 0> | 250.0 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 153.1 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 153.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 1 0> | 250.0 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 250.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 88.4 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 265.1 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 88.4 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 125.0 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 265.1 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 125.0 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 265.1 |
CaF2 (mp-2741) | <1 1 1> | <1 0 0> | 265.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm(GdS2)2 (mp-676424) | 0.1047 | 0.027 | 3 |
Nd(SmSb)3 (mp-675554) | 0.0448 | 0.039 | 3 |
Tb2SmS4 (mp-38931) | 0.0990 | 0.062 | 3 |
Sm(DyS2)2 (mp-34987) | 0.1112 | 0.070 | 3 |
Ca(Sm2Se3)4 (mp-34196) | 0.1116 | 0.061 | 3 |
Nd4Sb3 (mp-530) | 0.0194 | 0.000 | 2 |
Pr4Bi3 (mp-23314) | 0.0037 | 0.011 | 2 |
Nd4Bi3 (mp-23175) | 0.0125 | 0.000 | 2 |
La4Sb3 (mp-1223) | 0.0064 | 0.000 | 2 |
Ce4As3 (mp-21011) | 0.0202 | 0.028 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Sb |
Final Energy/Atom-5.5126 eV |
Corrected Energy-77.1759 eV
-77.1759 eV = -77.1759 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)