Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.724 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.580 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 316.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 83.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 190.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 253.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 190.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 63.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 104.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 46.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 230.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 190.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 209.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 250.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 190.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 167.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 313.4 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 209.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 126.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 250.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 138.3 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 286.3 |
GaSe (mp-1943) | <1 1 0> | <0 1 1> | 235.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 276.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 126.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 322.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 190.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 95.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 138.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 138.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 230.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 253.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 253.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 190.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 316.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 83.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 184.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 209.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 167.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 316.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 138.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 167.1 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 235.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 230.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 167.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 138.3 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 235.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 230.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 286.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 184.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl2SO4 (mp-4112) | 0.1693 | 0.000 | 3 |
Cs2SeO4 (mp-562442) | 0.1937 | 0.000 | 3 |
Rb2MnO4 (mp-541438) | 0.1563 | 0.000 | 3 |
Rb2CrO4 (mp-19643) | 0.1409 | 0.000 | 3 |
K2FeO4 (mp-19320) | 0.1758 | 0.000 | 3 |
KBaPO4 (mp-6812) | 0.2520 | 0.000 | 4 |
RbBaPO4 (mp-17832) | 0.2840 | 0.000 | 4 |
K2NClO3 (mp-559513) | 0.3389 | 0.853 | 4 |
BaTlVO4 (mp-561195) | 0.3869 | 0.000 | 4 |
RbBaMnO4 (mp-19681) | 0.3782 | 0.000 | 4 |
NdH4S2NO8 (mp-774927) | 0.6812 | 0.000 | 5 |
CaGdTh(PO4)3 (mp-695308) | 0.6104 | 0.013 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Be_sv Tl_d F |
Final Energy/Atom-4.7447 eV |
Corrected Energy-132.8503 eV
-132.8503 eV = -132.8503 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)