Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.203 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd10S19 + Ag + Nd2S3 |
Band Gap1.624 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 221.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 146.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 293.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 219.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 104.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 104.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 208.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 147.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 293.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 295.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 208.1 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 293.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 219.8 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 104.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 219.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 208.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 293.0 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 208.1 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 208.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 293.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 73.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 104.1 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 127.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 104.1 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 127.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 221.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 219.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 73.3 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 104.1 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 146.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 73.3 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 104.1 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 104.1 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 219.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 146.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 1> | 255.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 208.1 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 293.0 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 1> | 208.1 |
Si (mp-149) | <1 0 0> | <0 0 1> | 146.5 |
Au (mp-81) | <1 0 0> | <1 0 1> | 104.1 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 73.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 104.5 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 293.0 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 147.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.23898 | 0.17670 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.17670 | 0.23898 | 0.00000 |
-0.20295 | 0.20294 | 0.00000 | 0.00000 | 0.00000 | 0.44645 |
Piezoelectric Modulus ‖eij‖max0.53075 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.77 | -0.00 | 0.00 |
0.00 | 8.77 | 0.00 |
0.00 | 0.00 | 8.66 |
Dielectric Tensor εij (total) |
||
---|---|---|
26.56 | -0.00 | 0.00 |
0.00 | 26.56 | 0.00 |
0.00 | 0.00 | 28.33 |
Polycrystalline dielectric constant
εpoly∞
8.73
|
Polycrystalline dielectric constant
εpoly
27.15
|
Refractive Index n2.96 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce5AgS8 (mp-675643) | 0.0657 | 0.033 | 3 |
Pr5AgS8 (mp-34486) | 0.0350 | 0.022 | 3 |
La5AgS8 (mp-37478) | 0.0368 | 0.024 | 3 |
Sm5AgS8 (mp-37923) | 0.0432 | 0.022 | 3 |
Sm5AgSe8 (mp-38805) | 0.0680 | 0.024 | 3 |
Hf3N4 (mp-11660) | 0.3817 | 0.069 | 2 |
Zr3N4 (mp-11661) | 0.3857 | 0.045 | 2 |
Pr4As3 (mp-2365) | 0.3834 | 0.019 | 2 |
Eu4As3 (mp-20995) | 0.3836 | 0.000 | 2 |
La4As3 (mp-568959) | 0.3846 | 0.010 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Ag S |
Final Energy/Atom-6.0925 eV |
Corrected Energy-90.6033 eV
-90.6033 eV = -85.2957 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|