Final Magnetic Moment
0.491 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.177 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.99 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 71020 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 1 1> <0 0 1> 0.000 283.5
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.000 283.5
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.002 323.9
ZnO (mp-2133) <0 0 1> <0 0 1> 0.003 121.5
BN (mp-984) <0 0 1> <0 0 1> 0.004 283.5
AlN (mp-661) <0 0 1> <0 0 1> 0.015 162.0
Au (mp-81) <1 1 1> <0 0 1> 0.028 121.5
InP (mp-20351) <1 0 0> <0 0 1> 0.033 283.5
C (mp-48) <0 0 1> <0 0 1> 0.038 162.0
GaN (mp-804) <1 0 1> <0 0 1> 0.058 283.5
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.068 121.5
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.069 162.0
Ag (mp-124) <1 1 1> <0 0 1> 0.077 121.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.079 162.0
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.109 162.0
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.112 283.5
PbS (mp-21276) <1 1 0> <0 0 1> 0.149 202.5
InP (mp-20351) <1 1 0> <0 0 1> 0.156 202.5
PbS (mp-21276) <1 0 0> <0 0 1> 0.171 283.5
Au (mp-81) <1 0 0> <0 0 1> 0.180 283.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.184 283.5
MgO (mp-1265) <1 1 0> <0 0 1> 0.201 202.5
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.207 162.0
Cu (mp-30) <1 1 1> <0 0 1> 0.208 162.0
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.210 283.5
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.218 323.9
Ni (mp-23) <1 1 1> <0 0 1> 0.236 283.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.243 283.5
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.268 162.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.275 283.5
CdS (mp-672) <0 0 1> <0 0 1> 0.347 283.5
GaP (mp-2490) <1 1 1> <0 0 1> 0.351 162.0
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.376 283.5
CdS (mp-672) <1 0 0> <0 0 1> 0.401 323.9
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.407 121.5
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.443 323.9
Au (mp-81) <1 1 0> <0 0 1> 0.475 202.5
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.478 202.5
Mg (mp-153) <1 0 1> <0 0 1> 0.479 202.5
LiF (mp-1138) <1 0 0> <0 0 1> 0.487 202.5
CdS (mp-672) <1 1 0> <0 0 1> 0.510 243.0
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.514 283.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.519 121.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.521 283.5
Ge (mp-32) <1 0 0> <0 0 1> 0.533 202.5
Ni (mp-23) <1 0 0> <0 0 1> 0.537 121.5
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.572 283.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.578 283.5
GaAs (mp-2534) <1 0 0> <0 0 1> 0.598 202.5
Ni (mp-23) <1 1 0> <0 0 1> 0.601 202.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
80 18 2 0 -1 0
18 80 2 -0 1 0
2 2 3 0 0 0
0 -0 0 1 0 1
-1 1 0 0 1 0
0 0 0 1 0 31
Compliance Tensor Sij (10-12Pa-1)
13.4 -2.9 -6 -0.2 6.9 0
-2.9 13.4 -6 0.2 -6.9 0
-6 -6 335.1 0 0 0
-0.2 0.2 0 762.2 0 -13.8
6.9 -6.9 0 0 762.2 -0.4
0 0 0 -13.8 -0.4 32.7
Shear Modulus GV
16 GPa
Bulk Modulus KV
23 GPa
Shear Modulus GR
2 GPa
Bulk Modulus KR
3 GPa
Shear Modulus GVRH
9 GPa
Bulk Modulus KVRH
13 GPa
Elastic Anisotropy
34.71
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlSiTe3 (mp-31220) 0.2209 0.000 3
CrGeTe3 (mp-541449) 0.2486 0.260 3
VPS3 (mp-1078971) 0.2435 0.146 3
NiPS3 (mp-676040) 0.2350 0.080 3
CrGeTe3 (mp-1078220) 0.2430 0.260 3
GaAg(PSe3)2 (mp-7008) 0.5967 0.016 4
InCu(PSe3)2 (mp-22449) 0.4444 0.017 4
LiNi(PS3)2 (mp-557500) 0.5364 0.035 4
InAg(PSe3)2 (mp-20902) 0.5618 0.000 4
InAg(PS3)2 (mp-22661) 0.5921 0.000 4
IrS2 (mp-2833) 0.6269 0.000 2
Te2Ir (mp-569388) 0.6331 0.000 2
IrSe2 (mp-1361) 0.6297 0.000 2
Rh3Se8 (mp-1407) 0.6141 0.000 2
Rh3Se8 (mp-32861) 0.5848 0.007 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cr_pv Si Te
Final Energy/Atom
-5.0874 eV
Corrected Energy
-53.4060 eV
Uncorrected energy = -50.8740 eV Composition-based energy adjustment (-0.422 eV/atom x 6.0 atoms) = -2.5320 eV Corrected energy = -53.4060 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 626810
  • 626809
  • 62379
  • 71020
Submitted by
User remarks:
  • Chromium silicon telluride (1/1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)