Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.870 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 228.6 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 193.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 164.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 279.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 164.6 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 1> | 323.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 272.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 239.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 83.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 134.3 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 147.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 279.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 332.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 272.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 242.0 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 0> | 234.3 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 1> | 258.4 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 164.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 307.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 302.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 309.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 239.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 223.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 125.7 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 109.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 159.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 164.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 279.2 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 228.6 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 109.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 136.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 83.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 228.6 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 1> | 323.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 125.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 211.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 1> | 258.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 307.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 223.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 239.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 171.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 159.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 102.6 |
CdS (mp-672) | <1 1 1> | <1 -1 1> | 258.4 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 228.6 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 164.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 211.8 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 239.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 196.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 272.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zr10HN8 (mp-674456) | 0.1228 | 0.005 | 3 |
Ca28(Yb5S16)3 (mp-685526) | 0.1043 | 0.147 | 3 |
Li6FeCl8 (mp-28828) | 0.1893 | 0.092 | 3 |
Li6MgBr8 (mp-29008) | 0.1905 | 0.020 | 3 |
Li6VCl8 (mp-29250) | 0.1893 | 0.013 | 3 |
Li3VCr3O8 (mp-764983) | 0.2640 | 0.037 | 4 |
Li3VCr3O8 (mp-771672) | 0.2634 | 0.038 | 4 |
Li3Cr2(FeO4)2 (mp-780017) | 0.2550 | 1.106 | 4 |
Li2Ti4VO8 (mp-768018) | 0.1953 | 0.105 | 4 |
Li3VFe3O8 (mp-773273) | 0.2517 | 0.072 | 4 |
Fe7O8 (mp-705548) | 0.1794 | 0.099 | 2 |
Zr10C9 (mp-684623) | 0.1164 | 0.000 | 2 |
Fe12O13 (mp-764326) | 0.2088 | 0.083 | 2 |
Fe7O8 (mp-32939) | 0.1834 | 0.099 | 2 |
Ni9O10 (mp-656884) | 0.1572 | 0.047 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.6404 | 0.882 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv Ti_pv N |
Final Energy/Atom-9.7100 eV |
Corrected Energy-187.7383 eV
Uncorrected energy = -184.4893 eV
Composition-based energy adjustment (-0.361 eV/atom x 9.0 atoms) = -3.2490 eV
Corrected energy = -187.7383 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)