Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3ErBr6 |
Band Gap4.359 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 247.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 247.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 165.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 165.0 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 190.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 90.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 247.5 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 188.4 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 271.7 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 271.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 247.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 247.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 165.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 181.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 181.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 165.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 90.6 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 271.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 165.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 247.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 247.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 165.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 157.8 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 181.1 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 190.1 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 165.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 247.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 247.5 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 271.7 |
SiC (mp-11714) | <1 1 1> | <0 1 0> | 271.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 247.5 |
Au (mp-81) | <1 1 0> | <0 0 1> | 247.5 |
Au (mp-81) | <1 1 1> | <0 0 1> | 247.5 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 247.5 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 165.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 247.5 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 190.1 |
TiO2 (mp-390) | <1 1 1> | <0 1 0> | 271.7 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 271.7 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 157.8 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 190.1 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 165.0 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 165.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3FeF6 (mp-776784) | 0.4440 | 0.088 | 3 |
Li3ScCl6 (mp-686004) | 0.1866 | 0.012 | 3 |
Na3GdI6 (mp-675237) | 0.1996 | 0.000 | 3 |
Li3VF6 (mp-765499) | 0.4490 | 0.086 | 3 |
Li3InCl6 (mp-676109) | 0.2673 | 0.000 | 3 |
Li2Mn3(FeO4)3 (mp-767665) | 0.4544 | 0.098 | 4 |
Li2Mn3Cr3O12 (mp-850956) | 0.4226 | 0.075 | 4 |
Li2Ti3V3O12 (mp-763640) | 0.4025 | 0.093 | 4 |
LiAl2FeO6 (mp-770071) | 0.4598 | 0.131 | 4 |
LiV2CrO6 (mp-849360) | 0.4748 | 0.106 | 4 |
Ho2Se3 (mp-9824) | 0.1279 | 0.000 | 2 |
Sc2S3 (mp-684969) | 0.1155 | 0.004 | 2 |
Sc2S3 (mp-401) | 0.1262 | 0.000 | 2 |
Er2Te3 (mp-14643) | 0.2168 | 0.000 | 2 |
Er2Se3 (mp-209) | 0.1264 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Er_3 Br |
Final Energy/Atom-3.6918 eV |
Corrected Energy-73.8356 eV
-73.8356 eV = -73.8356 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)