material

ScCo2Sn

ID:

mp-3791

DOI:

10.17188/1207437


Tags: Cobalt scandium tin (2/1/1)

Material Details

Final Magnetic Moment
1.019 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.414 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.80 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 102646 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 0 0> <1 0 0> 0.000 38.6
CdSe (mp-2691) <1 1 0> <1 1 0> 0.000 54.6
CdSe (mp-2691) <1 1 1> <1 1 1> 0.000 66.9
CsI (mp-614603) <1 0 0> <1 0 0> 0.000 308.8
BN (mp-984) <0 0 1> <1 1 1> 0.002 267.4
GaSb (mp-1156) <1 0 0> <1 0 0> 0.003 38.6
GaSb (mp-1156) <1 1 0> <1 1 0> 0.003 54.6
GaSb (mp-1156) <1 1 1> <1 1 1> 0.003 66.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.005 308.8
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.011 66.9
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.011 66.9
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.011 154.4
PbSe (mp-2201) <1 0 0> <1 0 0> 0.015 38.6
PbSe (mp-2201) <1 1 0> <1 1 0> 0.016 54.6
PbSe (mp-2201) <1 1 1> <1 1 1> 0.016 66.9
SiC (mp-8062) <1 0 0> <1 0 0> 0.027 38.6
SiC (mp-7631) <1 1 0> <1 1 0> 0.027 163.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.028 54.6
CdS (mp-672) <0 0 1> <1 1 1> 0.034 200.6
C (mp-66) <1 1 0> <1 1 0> 0.035 54.6
C (mp-66) <1 1 1> <1 1 1> 0.036 66.9
TePb (mp-19717) <1 0 0> <1 0 0> 0.036 347.4
GaSe (mp-1943) <0 0 1> <1 1 1> 0.037 200.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.038 308.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.038 308.8
AlN (mp-661) <0 0 1> <1 0 0> 0.041 270.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.044 115.8
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.049 66.9
LiF (mp-1138) <1 1 1> <1 1 1> 0.050 200.6
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.050 218.3
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.052 163.8
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.055 308.8
Mg (mp-153) <0 0 1> <1 0 0> 0.055 308.8
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.058 38.6
Ag (mp-124) <1 0 0> <1 0 0> 0.060 154.4
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.061 54.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.061 193.0
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.062 66.9
Ag (mp-124) <1 1 0> <1 1 0> 0.063 218.3
Ag (mp-124) <1 1 1> <1 1 1> 0.064 267.4
InAs (mp-20305) <1 0 0> <1 0 0> 0.073 38.6
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.073 308.8
Cu (mp-30) <1 0 0> <1 1 0> 0.073 272.9
InAs (mp-20305) <1 1 0> <1 1 0> 0.076 54.6
InAs (mp-20305) <1 1 1> <1 1 1> 0.077 66.9
SiC (mp-7631) <1 0 1> <1 0 0> 0.089 193.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.106 347.4
ZnO (mp-2133) <1 0 0> <1 0 0> 0.124 193.0
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.126 193.0
InSb (mp-20012) <1 0 0> <1 0 0> 0.129 347.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
214 97 97 0 0 0
97 214 97 0 0 0
97 97 214 0 0 0
0 0 0 87 0 0
0 0 0 0 87 0
0 0 0 0 0 87
Compliance Tensor Sij (10-12Pa-1)
6.5 -2 -2 0 0 0
-2 6.5 -2 0 0 0
-2 -2 6.5 0 0 0
0 0 0 11.5 0 0
0 0 0 0 11.5 0
0 0 0 0 0 11.5
Shear Modulus GV
76 GPa
Bulk Modulus KV
136 GPa
Shear Modulus GR
73 GPa
Bulk Modulus KR
136 GPa
Shear Modulus GVRH
74 GPa
Bulk Modulus KVRH
136 GPa
Elastic Anisotropy
0.19
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiGaCo2 (mp-20145) 0.0000 0.000 3
CeCd2Ag (mp-31173) 0.0000 0.042 3
AlVCo2 (mp-4955) 0.0000 0.000 3
MnAlPd2 (mp-10891) 0.0000 0.030 3
ScInNi2 (mp-21301) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Ca3Tl (mp-30482) 0.0000 0.046 2
PrMg3 (mp-428) 0.0000 0.023 2
K3Sb (mp-10159) 0.0000 0.028 2
LiCd (mp-1437) 0.0000 0.000 2
DyMg3 (mp-1546) 0.0000 0.000 2
Sr (mp-95) 0.0000 0.013 1
Yb (mp-71) 0.0000 0.017 1
Dy (mp-10751) 0.0000 0.147 1
Li (mp-135) 0.0000 0.005 1
La (mp-10023) 0.0000 0.134 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Co Sn_d
Final Energy/Atom
-6.5494 eV
Corrected Energy
-26.1974 eV
Uncorrected energy = -26.1974 eV Corrected energy = -26.1974 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106492
  • 102646
Submitted by
User remarks:
  • Cobalt scandium tin (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)