Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.303 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.204 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2CN2 + C |
Band Gap5.354 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImm2 [44] |
HallI 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 179.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 213.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 143.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 30.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 209.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 133.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 166.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 145.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 210.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 152.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 335.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 327.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 119.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 213.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 182.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 133.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 149.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 177.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 152.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 133.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 166.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 71.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 214.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 158.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 266.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 209.9 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 119.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 182.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 210.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 143.0 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 237.0 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 342.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 182.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 210.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 90.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 309.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 237.0 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 284.1 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 238.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 214.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 190.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 76.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 119.9 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 119.9 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 284.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 262.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 327.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 284.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 213.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 329.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na(NO)2 (mp-675301) | 0.6760 | 0.714 | 3 |
LiNO3 (mp-696822) | 0.6825 | 1.117 | 3 |
NaCN (mp-30053) | 0.5911 | 0.200 | 3 |
KCN (mp-35035) | 0.1256 | 0.139 | 3 |
SrC2 (mp-1008776) | 0.7437 | 0.202 | 2 |
CaC2 (mp-1575) | 0.6978 | 0.014 | 2 |
BaC2 (mp-10293) | 0.7081 | 0.147 | 2 |
SrC2 (mp-10497) | 0.5841 | 0.053 | 2 |
ThC2 (mp-570108) | 0.4645 | 0.323 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv C N |
Final Energy/Atom-6.4706 eV |
Corrected Energy-19.4118 eV
-19.4118 eV = -19.4118 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)