material

Mg(AlSi)2

ID:

mp-3833

DOI:

10.17188/1207508


Tags: Magnesium dialuminium disilicide - U1

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.007 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg2Si + Si + Al
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 156100 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.000 274.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.003 187.7
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.005 274.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.007 101.1
Ge (mp-32) <1 1 1> <0 0 1> 0.009 57.8
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.009 245.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.012 57.8
MgO (mp-1265) <1 1 0> <1 1 0> 0.013 283.4
SiC (mp-7631) <1 0 0> <1 0 0> 0.015 327.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.016 57.8
C (mp-48) <1 0 1> <1 0 0> 0.017 218.2
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.031 247.0
CsI (mp-614603) <1 0 0> <1 1 1> 0.036 247.0
AlN (mp-661) <1 1 0> <1 0 1> 0.037 246.9
BaF2 (mp-1029) <1 0 0> <1 1 1> 0.038 197.6
SrTiO3 (mp-4651) <0 0 1> <1 1 1> 0.038 247.0
GaAs (mp-2534) <1 1 1> <0 0 1> 0.040 57.8
CaF2 (mp-2741) <1 1 0> <1 0 1> 0.042 216.0
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.045 216.6
Ni (mp-23) <1 0 0> <1 1 1> 0.045 49.4
C (mp-48) <0 0 1> <0 0 1> 0.046 101.1
SrTiO3 (mp-4651) <1 1 0> <1 1 1> 0.046 247.0
Cu (mp-30) <1 1 1> <0 0 1> 0.047 274.4
GaN (mp-804) <1 1 1> <1 0 0> 0.050 245.5
GaSe (mp-1943) <1 1 0> <1 1 0> 0.053 236.2
GaN (mp-804) <1 0 0> <1 0 0> 0.055 136.4
GaP (mp-2490) <1 1 0> <1 0 1> 0.056 216.0
InSb (mp-20012) <1 1 1> <0 0 1> 0.061 231.0
InSb (mp-20012) <1 1 0> <1 1 0> 0.062 189.0
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.067 185.2
NdGaO3 (mp-3196) <1 1 0> <1 1 1> 0.069 247.0
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.070 57.8
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.072 277.8
AlN (mp-661) <1 0 0> <1 0 0> 0.072 109.1
Au (mp-81) <1 1 1> <0 0 1> 0.072 274.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.075 189.0
CdTe (mp-406) <1 1 1> <0 0 1> 0.076 231.0
Te2W (mp-22693) <0 1 0> <0 0 1> 0.078 216.6
SiC (mp-11714) <1 1 1> <0 0 1> 0.081 332.1
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.083 81.8
TiO2 (mp-390) <1 0 0> <0 0 1> 0.084 259.9
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.085 327.3
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.088 216.6
C (mp-66) <1 1 0> <0 0 1> 0.089 72.2
InAs (mp-20305) <1 1 0> <0 0 1> 0.089 216.6
SiC (mp-8062) <1 1 0> <0 0 1> 0.090 216.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.090 43.3
Al (mp-134) <1 1 0> <0 0 1> 0.091 115.5
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.091 274.4
YAlO3 (mp-3792) <1 1 0> <1 0 1> 0.091 339.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
128 57 32 -4 0 0
57 128 32 4 0 0
32 32 93 0 0 0
-4 4 0 28 0 0
0 0 0 0 28 -4
0 0 0 0 -4 36
Compliance Tensor Sij (10-12Pa-1)
10.2 -4.1 -2.1 2.2 0 0
-4.1 10.2 -2.1 -2.2 0 0
-2.1 -2.1 12.1 0 0 0
2.2 -2.2 0 36.6 0 0
0 0 0 0 36.6 4.4
0 0 0 0 4.4 28.7
Shear Modulus GV
33 GPa
Bulk Modulus KV
66 GPa
Shear Modulus GR
32 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
33 GPa
Bulk Modulus KVRH
64 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr(CdAs)2 (mp-7771) 0.0692 0.000 3
Eu(CdAs)2 (mp-1070314) 0.0340 0.000 3
Eu(CdP)2 (mp-22609) 0.0527 0.000 3
Li2MnO2 (mp-19279) 0.0810 0.010 3
Eu(CdSb)2 (mp-19774) 0.0782 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.2087 0.040 4
LiFeCuS2 (mp-755288) 0.2689 0.124 4
Pu2O3 (mp-908430) 0.2677 0.073 2
Mg3As2 (mp-7891) 0.1725 0.018 2
Pu2O3 (mp-21423) 0.2172 0.073 2
Mg3Sb2 (mp-2646) 0.2183 0.000 2
Sc2O3 (mp-13060) 0.2680 0.132 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Al Si
Final Energy/Atom
-3.9955 eV
Corrected Energy
-19.9777 eV
-19.9777 eV = -19.9777 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 156101
  • 156100
Submitted by
User remarks:
  • Magnesium dialuminium disilicide - U1

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)