material

Li5ReN4

ID:

mp-3838

DOI:

10.17188/1207513


Tags: Pentalithium tetranitridorhenate(VII)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.816 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.14 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.847 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmmn [59]
Hall
P 2 2ab 1ab
Point Group
mmm
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.005 197.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.005 229.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.005 229.9
Al (mp-134) <1 1 1> <0 0 1> 0.009 197.1
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.018 164.2
PbS (mp-21276) <1 0 0> <1 0 0> 0.025 180.3
Ag (mp-124) <1 0 0> <1 0 0> 0.025 225.3
Au (mp-81) <1 0 0> <1 0 0> 0.029 225.3
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.030 262.8
CdWO4 (mp-19387) <1 1 0> <1 1 1> 0.030 324.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.032 90.1
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.032 225.3
Te2W (mp-22693) <0 1 0> <1 1 1> 0.035 324.7
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.036 167.3
Ni (mp-23) <1 0 0> <0 0 1> 0.041 98.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.043 164.2
GaSe (mp-1943) <0 0 1> <0 1 1> 0.047 187.0
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.050 225.3
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.050 164.2
GaN (mp-804) <1 1 0> <0 0 1> 0.065 295.6
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.074 278.8
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.078 98.5
MgO (mp-1265) <1 1 1> <1 0 1> 0.080 278.8
C (mp-48) <0 0 1> <0 1 0> 0.080 166.3
Cu (mp-30) <1 0 0> <1 0 0> 0.083 225.3
CaF2 (mp-2741) <1 1 0> <1 1 1> 0.083 129.9
Ag (mp-124) <1 1 0> <1 1 1> 0.084 194.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.084 262.8
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.085 225.3
NdGaO3 (mp-3196) <1 0 0> <1 1 1> 0.086 129.9
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.086 262.8
C (mp-48) <1 0 0> <1 1 1> 0.087 194.8
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.087 259.7
InSb (mp-20012) <1 1 0> <0 1 1> 0.088 187.0
ZrO2 (mp-2858) <1 1 1> <1 1 1> 0.089 259.7
CdTe (mp-406) <1 1 0> <0 1 1> 0.090 187.0
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.090 328.5
GaN (mp-804) <1 0 0> <1 0 1> 0.097 167.3
Te2Mo (mp-602) <1 0 0> <1 1 1> 0.098 324.7
GaP (mp-2490) <1 1 0> <1 1 1> 0.099 129.9
CsI (mp-614603) <1 1 0> <1 1 1> 0.100 259.7
ZnO (mp-2133) <0 0 1> <1 0 0> 0.100 225.3
Ni (mp-23) <1 1 0> <0 1 1> 0.103 140.3
InP (mp-20351) <1 0 0> <1 0 0> 0.107 180.3
Au (mp-81) <1 1 0> <1 1 1> 0.110 194.8
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.112 262.8
Mg (mp-153) <1 0 0> <1 0 1> 0.113 167.3
NdGaO3 (mp-3196) <0 1 0> <1 1 1> 0.128 129.9
Si (mp-149) <1 1 1> <0 0 1> 0.143 262.8
AlN (mp-661) <0 0 1> <0 0 1> 0.146 164.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
129 48 37 0 0 0
48 142 34 0 0 0
37 34 135 0 0 0
0 0 0 56 0 0
0 0 0 0 33 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
9.3 -2.7 -1.9 0 0 0
-2.7 8.3 -1.4 0 0 0
-1.9 -1.4 8.3 0 0 0
0 0 0 18 0 0
0 0 0 0 30.3 0
0 0 0 0 0 20.5
Shear Modulus GV
47 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
45 GPa
Bulk Modulus KR
71 GPa
Shear Modulus GVRH
46 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.24

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
12
U Values
--
Pseudopotentials
VASP PAW: Li_sv N Re_pv
Final Energy/Atom
-6.1953 eV
Corrected Energy
-123.9056 eV
-123.9056 eV = -123.9056 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations

User Data

dtu

Authors:
name conditions value ref
band gap
type
indirect
method
Kohn-Sham
functional
GLLB-SC
3.27 eV
band gap
type
direct
method
Kohn-Sham
functional
GLLB-SC
3.27 eV
band gap
type
indirect
method
quasiparticle
functional
GLLB-SC
4.43 eV
band gap
type
direct
method
quasiparticle
functional
GLLB-SC
4.43 eV
derivative discontinuity
functional
GLLB-SC
1.16 eV

Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 92467
  • 92468

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)