material

MgP4

ID:

mp-384

DOI:

10.17188/1207516


Tags: Magnesium phosphide (1/4)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.306 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.667 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 113 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe3O4 (mp-19306) <1 0 0> <1 0 -1> 0.000 218.5
MoS2 (mp-1434) <1 0 0> <1 0 0> 0.007 272.2
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.008 212.5
MgO (mp-1265) <1 0 0> <1 0 -1> 0.011 218.5
Ge (mp-32) <1 0 0> <0 0 1> 0.033 132.8
SiC (mp-7631) <1 0 0> <1 0 0> 0.034 233.3
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.034 106.3
SiC (mp-8062) <1 1 0> <0 1 0> 0.037 272.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.039 116.7
LiGaO2 (mp-5854) <1 0 0> <1 1 1> 0.039 318.0
GaAs (mp-2534) <1 0 0> <0 0 1> 0.040 132.8
CdS (mp-672) <0 0 1> <1 1 0> 0.042 275.3
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.042 194.4
LiF (mp-1138) <1 0 0> <0 0 1> 0.042 132.8
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.046 132.8
PbS (mp-21276) <1 0 0> <1 0 -1> 0.046 218.5
GaSe (mp-1943) <1 0 0> <1 0 0> 0.050 272.2
GdScO3 (mp-5690) <1 0 0> <1 1 -1> 0.050 234.3
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.051 132.8
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.052 272.9
MgF2 (mp-1249) <1 0 0> <0 1 1> 0.056 188.7
WS2 (mp-224) <1 0 1> <1 0 0> 0.058 233.3
GaSb (mp-1156) <1 0 0> <0 0 1> 0.061 345.4
YAlO3 (mp-3792) <1 0 0> <0 1 1> 0.067 283.1
SiC (mp-8062) <1 0 0> <1 1 1> 0.067 190.8
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.067 311.1
NaCl (mp-22862) <1 1 0> <1 1 1> 0.069 318.0
Mg (mp-153) <1 0 1> <1 0 -1> 0.077 131.1
BaTiO3 (mp-5986) <1 1 1> <1 0 -1> 0.080 87.4
PbSe (mp-2201) <1 0 0> <0 0 1> 0.081 345.4
ZrO2 (mp-2858) <0 1 1> <0 1 1> 0.081 235.9
LiGaO2 (mp-5854) <0 1 1> <1 0 -1> 0.084 43.7
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.085 350.9
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.086 311.1
Cu (mp-30) <1 1 0> <1 0 -1> 0.087 131.1
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.101 311.1
CaCO3 (mp-3953) <1 0 0> <1 0 -1> 0.103 87.4
Mg (mp-153) <1 1 1> <0 0 1> 0.105 239.1
TiO2 (mp-2657) <1 0 0> <1 0 1> 0.106 150.8
AlN (mp-661) <1 1 1> <1 1 1> 0.109 254.4
MgF2 (mp-1249) <1 1 1> <0 1 0> 0.111 272.9
CdWO4 (mp-19387) <1 1 0> <0 1 1> 0.114 283.1
Fe2O3 (mp-24972) <1 0 1> <1 0 1> 0.114 150.8
CdS (mp-672) <1 0 1> <1 0 -1> 0.118 131.1
Cu (mp-30) <1 0 0> <0 0 1> 0.125 26.6
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.126 311.1
InP (mp-20351) <1 1 0> <1 0 -1> 0.126 305.9
Ni (mp-23) <1 0 0> <0 0 1> 0.128 212.5
TbScO3 (mp-31119) <1 0 0> <1 1 -1> 0.132 234.3
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.141 53.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
123 37 34 0 11 0
37 96 38 0 -1 0
34 38 90 0 4 0
0 0 0 43 0 2
11 -1 4 0 32 0
0 0 0 2 0 47
Compliance Tensor Sij (10-12Pa-1)
9.9 -2.9 -2.4 0 -3.1 0
-2.9 13.4 -4.6 0 2 0
-2.4 -4.6 13.9 0 -1.2 0
0 0 0 23.3 0 -0.9
-3.1 2 -1.2 0 32.2 0
0 0 0 -0.9 0 21.4
Shear Modulus GV
38 GPa
Bulk Modulus KV
58 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
57 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
58 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.24

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
10.22 0.00 0.57
0.00 11.36 0.00
0.57 0.00 9.28
Dielectric Tensor εij (total)
11.92 0.00 0.36
0.00 14.70 0.00
0.36 0.00 14.32
Polycrystalline dielectric constant εpoly
(electronic contribution)
10.29
Polycrystalline dielectric constant εpoly
(total)
13.65
Refractive Index n
3.21
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiFeF3 (mp-849232) 0.6010 0.032 3
Ge3Rh2Se3 (mp-976401) 0.6086 0.000 3
Ge3Ir2Se3 (mp-975924) 0.5807 0.000 3
Co2(GeS)3 (mp-2956) 0.5956 0.000 3
AlSiP3 (mp-5168) 0.5847 0.007 3
LiVCuO4 (mp-771628) 0.6603 0.107 4
Zn2BiWO6 (mvc-5039) 0.6328 0.099 4
LiMnOF2 (mp-766924) 0.5576 0.097 4
LiMnOF2 (mp-765076) 0.6496 0.080 4
Zn2CoWO6 (mvc-6162) 0.6473 0.057 4
MgAs4 (mp-7623) 0.3484 0.000 2
Te2Ir (mp-569322) 0.6220 0.012 2
FeP4 (mp-568328) 0.6196 0.014 2
ZnP4 (mp-14587) 0.1836 0.063 2
CdP4 (mp-7904) 0.1377 0.011 2
Li4Fe2TeWO12 (mp-768021) 0.6691 0.083 5
Li4Cr2TeWO12 (mp-775566) 0.6781 0.080 5
Li4Mn2TeWO12 (mp-768044) 0.6798 0.058 5
Li4TiMn(WO6)2 (mp-770980) 0.6967 0.033 5
Li4V2CrTeO12 (mp-775632) 0.6564 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv P
Final Energy/Atom
-4.9568 eV
Corrected Energy
-49.5681 eV
-49.5681 eV = -49.5681 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 23555
  • 42030
  • 113
Submitted by
User remarks:
  • Magnesium phosphide (1/4)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)