Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.304 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.263 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 243.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 196.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 336.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 112.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 252.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 224.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 168.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 252.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 308.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 196.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 336.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 121.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 84.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 140.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 364.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 280.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 224.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 168.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 308.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 196.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 112.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 84.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 112.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 336.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 308.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 196.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 308.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 364.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 196.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 112.1 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 121.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 308.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 308.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 196.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 112.1 |
MoS2 (mp-1434) | <1 1 1> | <1 0 1> | 124.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 112.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 28.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 252.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 364.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 168.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 224.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 336.4 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 364.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 252.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 140.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.25 | -0.00 | -0.00 |
-0.00 | 3.25 | -0.00 |
-0.00 | -0.00 | 3.22 |
Dielectric Tensor εij (total) |
||
---|---|---|
20.43 | -0.00 | -0.00 |
-0.00 | 20.43 | -0.00 |
-0.00 | -0.00 | 10.77 |
Polycrystalline dielectric constant
εpoly∞
3.24
|
Polycrystalline dielectric constant
εpoly
17.21
|
Refractive Index n1.80 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3(AsO4)2 (mp-9783) | 0.2668 | 0.000 | 3 |
K3Mn2O8 (mp-510713) | 0.1407 | 0.006 | 3 |
Ba3Cr2O8 (mp-18913) | 0.2567 | 0.002 | 3 |
Ba3Mn2O8 (mp-19188) | 0.2329 | 0.000 | 3 |
Sr3(PO4)2 (mp-4632) | 0.1999 | 0.000 | 3 |
K2Be2PbF8 (mp-7385) | 0.3103 | 0.003 | 4 |
K3MnCrO8 (mp-761384) | 0.2169 | 0.010 | 4 |
K2SrBe2F8 (mp-12626) | 0.3589 | 0.003 | 4 |
K2Pb(SO4)2 (mp-21099) | 0.2912 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv P O |
Final Energy/Atom-7.1925 eV |
Corrected Energy-99.1207 eV
-99.1207 eV = -93.5024 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)