material

Ti2SnC

ID:

mp-3871

DOI:

10.17188/1207556


Tags: Titanium tin carbide (2/1/1) High pressure experimental phase

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.721 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaSe (mp-1943) <0 0 1> <0 0 1> 0.001 113.4
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.004 183.3
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.006 165.8
GaP (mp-2490) <1 0 0> <1 1 0> 0.008 151.8
CdS (mp-672) <0 0 1> <0 0 1> 0.009 61.1
Al (mp-134) <1 1 1> <0 0 1> 0.012 113.4
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.012 61.1
CaF2 (mp-2741) <1 0 0> <1 1 0> 0.012 151.8
Mg (mp-153) <0 0 1> <0 0 1> 0.028 8.7
InP (mp-20351) <1 1 1> <0 0 1> 0.029 61.1
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.034 165.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.038 218.2
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.039 139.6
PbSe (mp-2201) <1 1 1> <0 0 1> 0.040 270.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.049 113.4
Ga2O3 (mp-886) <1 1 1> <0 0 1> 0.051 253.1
BN (mp-984) <0 0 1> <0 0 1> 0.054 104.7
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.055 165.8
NdGaO3 (mp-3196) <1 1 0> <1 1 0> 0.064 303.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.065 113.4
Mg (mp-153) <1 1 0> <0 0 1> 0.068 87.3
GaSb (mp-1156) <1 1 1> <0 0 1> 0.073 270.5
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.082 219.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.084 8.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.085 8.7
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.088 157.1
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.089 157.1
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.090 139.6
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.097 270.5
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.105 52.4
CdSe (mp-2691) <1 1 1> <0 0 1> 0.106 270.5
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.113 340.3
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.122 219.0
ZnO (mp-2133) <1 1 1> <1 0 0> 0.124 219.0
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.131 279.3
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.141 340.3
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.152 303.5
GaTe (mp-542812) <0 0 1> <0 0 1> 0.153 305.4
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.154 139.6
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.156 113.4
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.157 113.4
InSb (mp-20012) <1 1 0> <1 0 1> 0.162 312.7
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.171 322.9
Si (mp-149) <1 0 0> <1 1 0> 0.172 151.8
LaF3 (mp-905) <1 1 0> <0 0 1> 0.172 279.3
CdTe (mp-406) <1 1 0> <1 0 1> 0.172 312.7
BN (mp-984) <1 0 1> <0 0 1> 0.175 218.2
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.176 279.3
CeO2 (mp-20194) <1 0 0> <1 1 0> 0.182 151.8
NaCl (mp-22862) <1 1 1> <0 0 1> 0.186 165.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
262 81 69 0 0 0
81 262 69 0 0 0
69 69 258 0 0 0
0 0 0 91 0 0
0 0 0 0 91 0
0 0 0 0 0 90
Compliance Tensor Sij (10-12Pa-1)
4.4 -1.1 -0.9 0 0 0
-1.1 4.4 -0.9 0 0 0
-0.9 -0.9 4.3 0 0 0
0 0 0 11 0 0
0 0 0 0 11 0
0 0 0 0 0 11.1
Shear Modulus GV
92 GPa
Bulk Modulus KV
135 GPa
Shear Modulus GR
92 GPa
Bulk Modulus KR
135 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
135 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zr2TlC (mp-1025524) 0.1408 0.000 3
Hf2SnC (mp-4893) 0.1424 0.000 3
Hf2TlC (mp-1078712) 0.0990 0.000 3
Hf2PbC (mp-1079076) 0.0519 0.000 3
Zr2PbC (mp-1079992) 0.0793 0.000 3
Co3H (mp-1025425) 0.4020 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: C Ti_pv Sn_d
Final Energy/Atom
-7.9780 eV
Corrected Energy
-63.8241 eV
-63.8241 eV = -63.8241 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 161063
  • 161064
  • 86812
  • 161065
  • 618806
Submitted by
User remarks:
  • Titanium tin carbide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)