material

Li3GaN2

ID:

mp-3887

DOI:

10.17188/1207576


Tags: Trilithium gallium dinitride High pressure experimental phase Gallium lithium nitride (1/3/2) Trilithium gallium nitride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.658 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.378 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Ia3 [206]
Hall
-I 2b 2c 3
Point Group
m3
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.006 132.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.014 187.2
GaN (mp-804) <1 1 0> <1 1 0> 0.024 264.8
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.027 280.8
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.030 264.8
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.037 280.8
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.037 280.8
CsI (mp-614603) <1 1 0> <1 1 0> 0.040 264.8
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.070 280.8
Mg (mp-153) <1 1 0> <1 1 0> 0.115 264.8
InAs (mp-20305) <1 0 0> <1 0 0> 0.166 187.2
TiO2 (mp-390) <1 1 0> <1 1 0> 0.173 264.8
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.184 187.2
SrTiO3 (mp-4651) <1 0 1> <1 1 0> 0.188 264.8
TiO2 (mp-390) <1 0 0> <1 0 0> 0.197 187.2
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.211 264.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.228 162.1
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.233 132.4
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.263 264.8
GaP (mp-2490) <1 1 1> <1 1 1> 0.295 162.1
GaP (mp-2490) <1 1 0> <1 1 0> 0.301 132.4
NaCl (mp-22862) <1 1 1> <1 0 0> 0.335 280.8
CdSe (mp-2691) <1 0 0> <1 0 0> 0.377 187.2
CdS (mp-672) <1 0 0> <1 0 0> 0.393 280.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.429 187.2
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.447 264.8
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.463 280.8
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.470 280.8
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.473 280.8
Al (mp-134) <1 1 1> <1 0 0> 0.493 280.8
PbSe (mp-2201) <1 0 0> <1 0 0> 0.499 187.2
GaAs (mp-2534) <1 1 1> <1 0 0> 0.514 280.8
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.532 264.8
MgF2 (mp-1249) <0 0 1> <1 1 0> 1.016 132.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
242 27 27 0 0 0
27 242 27 0 0 0
27 27 242 0 0 0
0 0 0 77 0 0
0 0 0 0 77 0
0 0 0 0 0 77
Compliance Tensor Sij (10-12Pa-1)
4.2 -0.4 -0.4 0 0 0
-0.4 4.2 -0.4 0 0 0
-0.4 -0.4 4.2 0 0 0
0 0 0 13 0 0
0 0 0 0 13 0
0 0 0 0 0 13
Shear Modulus GV
89 GPa
Bulk Modulus KV
99 GPa
Shear Modulus GR
87 GPa
Bulk Modulus KR
99 GPa
Shear Modulus GVRH
88 GPa
Bulk Modulus KVRH
99 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.16

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li5TiAs3 (mp-677039) 0.6717 0.006 3
Li3ScN2 (mp-542435) 0.3940 0.000 3
Li3FeN2 (mp-28628) 0.6898 0.000 3
Li3AlN2 (mp-13944) 0.3790 0.000 3
ZrBiO4 (mp-754588) 0.6768 0.079 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv N Ga_d
Final Energy/Atom
-4.7691 eV
Corrected Energy
-228.9177 eV
-228.9177 eV = -228.9177 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 419137
  • 25566
  • 634534
Submitted by
User remarks:
  • Trilithium gallium dinitride
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)