Final Magnetic Moment0.060 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.391 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd2S3 + Sm2S3 + NdS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 146.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 292.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 292.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 219.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 219.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 103.3 |
Al (mp-134) | <1 1 0> | <1 0 1> | 206.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.0 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 103.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 292.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 292.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 206.5 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 126.5 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 126.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 206.5 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 253.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 219.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 219.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 292.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 219.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 73.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 73.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 219.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 146.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 1> | 253.0 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 206.5 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 292.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 292.0 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 292.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 73.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 103.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.0 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 103.3 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 146.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 292.0 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 103.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 126.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 292.0 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 292.0 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 219.0 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 103.3 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 103.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 206.5 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 219.0 |
GaTe (mp-542812) | <1 0 1> | <1 0 0> | 292.2 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 219.0 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 292.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La5YbS8 (mp-676443) | 0.0719 | 0.017 | 3 |
Sm(GdS2)2 (mp-676424) | 0.0623 | 0.027 | 3 |
Pr2SmS4 (mp-37070) | 0.0284 | 0.038 | 3 |
Ca(PrTe2)2 (mp-37520) | 0.0555 | 0.015 | 3 |
Ce2SmS4 (mp-37045) | 0.0590 | 0.025 | 3 |
Gd3Se4 (mp-672292) | 0.0939 | 0.011 | 2 |
Ti4As3 (mp-567082) | 0.0944 | 0.004 | 2 |
Np3Se4 (mp-570181) | 0.0935 | 0.035 | 2 |
Ce4Sb3 (mp-20680) | 0.0938 | 0.001 | 2 |
Nd3S4 (mp-2656) | 0.0945 | 0.037 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Sm_3 S |
Final Energy/Atom-6.4122 eV |
Corrected Energy-95.0786 eV
-95.0786 eV = -89.7709 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)