MgTa2N3

ID:

mp-39105

DOI:

10.17188/1207613

Warnings: [?]
  1. Large change in a lattice parameter during relaxation.
  2. Large change in volume during relaxation.

Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-1.385 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.40 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mcm [193]
Hall
-P 6c 2
Point Group
6/mmm
Crystal System
hexagonal

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.001 166.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.007 219.6
InSb (mp-20012) <1 0 0> <1 0 0> 0.010 219.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.014 166.9
WS2 (mp-224) <0 0 1> <0 0 1> 0.015 166.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.019 109.8
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.020 54.9
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.022 286.1
C (mp-66) <1 1 1> <0 0 1> 0.034 286.1
BN (mp-984) <0 0 1> <0 0 1> 0.049 71.5
CdWO4 (mp-19387) <0 1 0> <1 0 1> 0.073 239.4
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.077 143.1
NaCl (mp-22862) <1 1 1> <0 0 1> 0.082 166.9
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.084 286.1
AlN (mp-661) <1 1 1> <1 1 0> 0.084 285.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.089 54.9
Ni (mp-23) <1 0 0> <1 0 0> 0.092 109.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.097 23.8
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.106 219.6
KCl (mp-23193) <1 1 1> <0 0 1> 0.108 71.5
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.110 164.7
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.179 219.6
AlN (mp-661) <0 0 1> <0 0 1> 0.179 214.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.190 219.6
MgO (mp-1265) <1 1 1> <0 0 1> 0.193 95.4
Au (mp-81) <1 0 0> <1 0 0> 0.232 274.5
Mg (mp-153) <1 1 0> <0 0 1> 0.235 143.1
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.238 47.7
Ni (mp-23) <1 1 0> <1 0 0> 0.239 329.4
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.243 109.8
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.250 23.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.257 286.1
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.275 119.2
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.290 219.6
LaF3 (mp-905) <1 0 1> <1 1 0> 0.305 285.3
InSb (mp-20012) <1 1 1> <0 0 1> 0.315 310.0
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.316 95.4
GaN (mp-804) <1 0 0> <1 0 1> 0.319 119.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.328 285.3
GaSe (mp-1943) <0 0 1> <0 0 1> 0.330 166.9
CdTe (mp-406) <1 1 1> <0 0 1> 0.364 310.0
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.382 310.0
TiO2 (mp-390) <1 0 1> <1 0 0> 0.420 274.5
GaN (mp-804) <0 0 1> <0 0 1> 0.446 166.9
ZnO (mp-2133) <1 0 0> <1 0 1> 0.478 119.7
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.481 214.6
C (mp-48) <0 0 1> <1 0 0> 0.497 274.5
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.502 357.7
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.547 285.3
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.582 109.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
555 150 131 -0 0 -0
150 555 131 0 -0 -0
131 131 555 0 0 -0
0 0 0 194 -0 -0
0 -0 0 -0 194 0
-0 -0 -0 0 0 203
Compliance Tensor Sij (10-12Pa-1)
2 -0.5 -0.4 0 0 0
-0.5 2 -0.4 0 0 0
-0.4 -0.4 2 0 0 0
0 0 0 5.2 0 0
0 0 0 0 5.2 0
0 0 0 0 0 4.9
Shear Modulus GV
202 GPa
Bulk Modulus KV
276 GPa
Shear Modulus GR
201 GPa
Bulk Modulus KR
276 GPa
Shear Modulus GVRH
201 GPa
Bulk Modulus KVRH
276 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na3Co2SbO6 (mp-19087) 0.4192 0.000 4
Na3Ni2SbO6 (mp-971678) 0.3970 0.000 4
Na3Co2SbO6 (mp-561940) 0.4705 0.098 4
Li3Fe(CoO3)2 (mp-761602) 0.4835 0.122 4
Li4TiCo3O8 (mp-770897) 0.4730 0.056 4
ZrAs (mp-1682) 0.0553 0.000 2
HfAs (mp-9954) 0.0496 0.000 2
TiAs (mp-1822) 0.0510 0.000 2
TiP (mp-739) 0.0490 0.000 2
HfP (mp-9953) 0.0580 0.000 2
MgMoN2 (mp-864954) 0.2252 0.000 3
Mn17Nb31N48 (mp-685705) 0.1981 0.206 3
YbScO2 (mp-769119) 0.0946 0.065 3
LiNbO2 (mp-3924) 0.1312 0.000 3
LiTiO2 (mp-755000) 0.2102 0.053 3
Xe (mp-979286) 0.6492 0.006 1
Sb (mp-632286) 0.7039 0.066 1
Na (mp-999501) 0.3812 0.129 1
Te (mp-105) 0.7422 0.042 1
Te (mp-570459) 0.7302 0.041 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv N Ta_pv
Final Energy/Atom
-9.5803 eV
Corrected Energy
-229.9273 eV
-229.9273 eV = -229.9273 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)