Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.888 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 212.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 159.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 200.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 250.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 265.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 115.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 273.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 212.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 150.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 212.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 265.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 250.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 146.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 115.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 300.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 273.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 265.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 300.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 250.4 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 146.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 250.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 250.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 200.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 250.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 265.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 250.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 150.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 265.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 318.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 318.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 250.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 182.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 273.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 219.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 200.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 106.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 292.1 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 318.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 250.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 200.3 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 150.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 200.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 318.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 50.1 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 250.4 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 230.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 150.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 50.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 219.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaWN3 (mp-989633) | 0.3615 | 0.011 | 3 |
LaMoN3 (mp-989631) | 0.3123 | 0.000 | 3 |
SrTcN3 (mp-989627) | 0.3366 | 0.000 | 3 |
SrReN3 (mp-989623) | 0.3872 | 0.000 | 3 |
LaTcN3 (mp-989619) | 0.3903 | 0.000 | 3 |
CaZn(SiO3)2 (mp-6693) | 0.3505 | 0.038 | 4 |
CaCr(SiO3)2 (mvc-5117) | 0.3149 | 0.040 | 4 |
NaFe(SiO3)2 (mp-510615) | 0.3441 | 0.000 | 4 |
CaAl2SiO6 (mp-1019587) | 0.3380 | 0.051 | 4 |
CaAl2SiO6 (mp-1019573) | 0.3471 | 0.017 | 4 |
Na5LiFe6(SiO3)12 (mp-767564) | 0.3582 | 0.182 | 5 |
Ca6Mg5Al2Si11O36 (mp-699405) | 0.3773 | 0.017 | 5 |
NaCaFe2(SiO3)4 (mvc-16542) | 0.3310 | 0.006 | 5 |
Ca2MgAl2(SiO4)3 (mp-677029) | 0.3052 | 0.019 | 5 |
Na9LiFe10(SiO3)20 (mp-775304) | 0.3597 | 0.003 | 5 |
Na2Ca6Mg7Fe(SiO3)16 (mp-745155) | 0.3522 | 0.031 | 6 |
NaCa3AlFe3(SiO3)8 (mp-743726) | 0.3662 | 0.158 | 6 |
NaCa3ScZn3(SiO3)8 (mp-693463) | 0.3334 | 0.029 | 6 |
NaCaScZn(SiO3)4 (mp-684991) | 0.3284 | 0.019 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.3207 | 0.025 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Sc_sv Al Si O |
Final Energy/Atom-7.8929 eV |
Corrected Energy-332.5705 eV
-332.5705 eV = -315.7156 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)