Final Magnetic Moment3.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.308 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaTiO3 + LaCrO3 |
Band Gap1.226 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmma [51] |
Hall-P 2a 2a |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 247.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 315.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 247.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 157.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 315.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 292.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 247.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 270.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 225.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 45.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 202.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 157.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 268.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 90.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 247.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 337.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 112.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 202.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 202.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 180.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 90.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 270.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 45.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 112.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 184.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 292.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 225.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 45.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 112.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 22.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 112.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 202.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 157.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 202.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 112.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 22.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 112.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 360.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 180.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 337.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 270.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 112.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 22.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 112.6 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 276.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 202.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 360.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 292.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 337.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsSrI3 (mp-998417) | 0.3793 | 0.032 | 3 |
RbSrCl3 (mp-998155) | 0.3787 | 0.041 | 3 |
CsSrBr3 (mp-998297) | 0.3785 | 0.020 | 3 |
RbAgBr3 (mp-998212) | 0.3815 | 0.000 | 3 |
RbPbCl3 (mp-998605) | 0.3816 | 0.038 | 3 |
Ba3CaRu2O9 (mp-12832) | 0.2894 | 0.000 | 4 |
Ba32Sb7Pb25O96 (mp-686499) | 0.2718 | 0.000 | 4 |
Ba3Ta2CdO9 (mp-554669) | 0.2709 | 0.000 | 4 |
Ba3CaIr2O9 (mp-13369) | 0.3049 | 0.030 | 4 |
Ba3MnNb2O9 (mp-638406) | 0.2907 | 0.000 | 4 |
Mn4N (mp-637576) | 0.4704 | 1.987 | 2 |
Fe2O3 (mp-1068212) | 0.4700 | 0.860 | 2 |
Fe4P (mp-20885) | 0.4748 | 0.686 | 2 |
Ni4O (mp-1094082) | 0.4759 | 1.616 | 2 |
Ni4N (mp-1094090) | 0.4759 | 0.067 | 2 |
BaLaTiCuO6 (mp-695277) | 0.0951 | 0.036 | 5 |
Ba3La2Ti3Cr2O15 (mp-705457) | 0.0628 | 0.028 | 5 |
BaLaTiCrO6 (mp-698663) | 0.0495 | 0.047 | 5 |
BaLa2TiCr2O9 (mp-743816) | 0.1190 | 0.325 | 5 |
BaLa2TiCr2O9 (mp-41732) | 0.0687 | 0.325 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.6770 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ba_sv La Ti_pv Cr_pv O |
Final Energy/Atom-8.0944 eV |
Corrected Energy-348.6833 eV
-348.6833 eV = -323.7764 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)