Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.422 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrTa2O6 + LiF |
Band Gap3.627 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 234.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 237.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 234.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 194.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 156.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 317.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 279.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 288.2 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 96.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 288.2 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 111.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 167.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 158.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 223.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 279.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 234.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 288.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 167.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 312.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 335.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 234.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 167.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 279.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 279.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 279.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 279.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 156.4 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 192.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 279.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 279.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 192.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 279.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 156.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 96.1 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 237.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 279.3 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 223.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 158.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 111.7 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 156.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 279.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 222.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 234.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 279.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 279.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 317.2 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 222.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 167.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 279.3 |
GaSe (mp-1943) | <1 1 0> | <0 1 0> | 234.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.63 | 0.00 | 0.00 |
0.00 | 4.50 | 0.00 |
0.00 | 0.00 | 4.41 |
Dielectric Tensor εij (total) |
||
---|---|---|
340.54 | 0.00 | 0.00 |
0.00 | 52.27 | 0.00 |
0.00 | 0.00 | 48.44 |
Polycrystalline dielectric constant
εpoly∞
4.51
|
Polycrystalline dielectric constant
εpoly
147.08
|
Refractive Index n2.12 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd2Os2O7 (mp-5950) | 0.5286 | 0.000 | 3 |
Cd2Ru2O7 (mp-505552) | 0.5295 | 0.000 | 3 |
Ca2Nb2O7 (mp-4155) | 0.5282 | 0.041 | 3 |
Nb2Cd2O7 (mp-5472) | 0.5284 | 0.010 | 3 |
Ca2Ru2O7 (mp-554638) | 0.5291 | 0.000 | 3 |
La2Nb2N2O5 (mp-775911) | 0.5729 | 0.071 | 4 |
Mn2Hg2SF6 (mp-600275) | 0.5817 | 0.465 | 4 |
Cu2Hg2SF6 (mp-6820) | 0.5283 | 0.000 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.5540 | 0.000 | 4 |
Ni2Hg2SF6 (mp-559259) | 0.5295 | 0.013 | 4 |
NaYb3Ti2(SbO7)2 (mp-695026) | 0.4241 | 0.074 | 5 |
NaCaNb2O6F (mp-42255) | 0.3716 | 0.005 | 5 |
KCaNb2O6F (mp-682067) | 0.2043 | 0.009 | 5 |
LiCaTa2O6F (mp-39511) | 0.4400 | 0.030 | 5 |
Sr3LiTa4(O6F)2 (mp-756170) | 0.4381 | 0.038 | 5 |
NaYbTiNbO6F (mp-684861) | 0.4269 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.5397 | 0.035 | 6 |
NaEuTiNbO6F (mp-43048) | 0.4623 | 0.019 | 6 |
NaCeTiNbO6F (mp-43055) | 0.5229 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.5365 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Li_sv Ta_pv O F |
Final Energy/Atom-8.3503 eV |
Corrected Energy-192.1352 eV
-192.1352 eV = -183.7077 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)