Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.639 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.295 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [161] |
HallR 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 1 1> | <0 0 1> | 201.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 268.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 67.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 201.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 67.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 201.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 201.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 201.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 268.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 67.2 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 201.7 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 268.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 67.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 67.2 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 268.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 268.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 201.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 268.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 268.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 67.2 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 67.2 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 268.9 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 268.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 201.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 201.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 268.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 268.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 201.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 201.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 268.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 201.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 201.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 201.7 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 67.2 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 268.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 268.9 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 268.9 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 67.2 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 67.2 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 201.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 67.2 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 67.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.47063 | -0.17841 |
-0.17841 | 0.17841 | 0.00000 | 0.47063 | 0.00000 | 0.00000 |
0.23071 | 0.23071 | -0.01639 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.53400 C/m2 |
Crystallographic Direction vmax |
---|
-0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.07 | 0.00 | -0.00 |
0.00 | 3.07 | -0.00 |
-0.00 | -0.00 | 3.19 |
Dielectric Tensor εij (total) |
||
---|---|---|
14.20 | 0.00 | -0.00 |
0.00 | 14.20 | -0.00 |
-0.00 | -0.00 | 11.22 |
Polycrystalline dielectric constant
εpoly∞
3.11
|
Polycrystalline dielectric constant
εpoly
13.20
|
Refractive Index n1.76 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni2(SO4)3 (mp-779193) | 0.4793 | 0.160 | 3 |
Ni2(SO4)3 (mp-770220) | 0.4698 | 0.212 | 3 |
NiP2O7 (mvc-15036) | 0.4565 | 0.227 | 3 |
Tl2Cr3O12 (mp-560926) | 0.4678 | 0.000 | 3 |
NiP2O7 (mp-540273) | 0.4759 | 0.227 | 3 |
K7Ta(SO4)6 (mp-17455) | 0.5204 | 0.000 | 4 |
K7Nb(SO4)6 (mp-17499) | 0.5129 | 0.000 | 4 |
NbPHO5 (mp-756508) | 0.5372 | 0.088 | 4 |
ZnP2(HO3)2 (mp-703593) | 0.4890 | 0.555 | 4 |
Fe2P3(HO3)3 (mp-25692) | 0.5344 | 0.384 | 4 |
Cr3O8 (mp-782705) | 0.7477 | 0.115 | 2 |
Cr5O12 (mp-19575) | 0.5617 | 0.142 | 2 |
Cr3O8 (mp-557959) | 0.7101 | 0.048 | 2 |
Mn3VTe2(PO4)6 (mp-782657) | 0.5870 | 0.086 | 5 |
Na2LaPS2O7 (mp-640915) | 0.5747 | 0.141 | 5 |
Mn2H8S3(NO6)2 (mp-762853) | 0.5880 | 0.001 | 5 |
FeH4S2NO8 (mp-703668) | 0.5760 | 0.000 | 5 |
TiMn3Te2(PO4)6 (mp-765557) | 0.5836 | 0.086 | 5 |
Na2Sc2P4H12C4O13 (mp-709352) | 0.6299 | 0.164 | 6 |
LiMnVP2(HO5)2 (mp-765378) | 0.6735 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-765074) | 0.6874 | 0.045 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6579 | 0.072 | 6 |
LiVCrP2(HO5)2 (mp-765078) | 0.6853 | 0.124 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.6706 | 0.050 | 7 |
SbTe6H12C4N(OF5)6 (mp-709549) | 0.6792 | 0.281 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv P H N O |
Final Energy/Atom-7.4208 eV |
Corrected Energy-343.3681 eV
-343.3681 eV = -326.5131 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)